Search found 206 matches
- Sat Nov 11, 2023 12:58 pm
- Forum: Techniques and Tools
- Topic: Piece cracked on slump
- Replies: 2
- Views: 20711
Piece cracked on slump
Third slump of a Deep Bowl and this happened.how to prevent this In future?
- Thu Apr 20, 2023 8:04 pm
- Forum: Techniques and Tools
- Topic: Brock Craig has passed on.
- Replies: 12
- Views: 26963
Re: Brock Craig has passed on.
So Jim what was the class you wanted to take from Brock? Was it one he was prevented from US travel to? You were on the board for a long enough time to 'know everything" weren't you? Perhaps the collective memories of old time board members could help? That Was the one, Irid on Irid with Avery...
- Tue Mar 28, 2023 5:07 pm
- Forum: Techniques and Tools
- Topic: Brock Craig has passed on.
- Replies: 12
- Views: 26963
Re: Brock Craig has passed on.
Very Sorry to hear this..one of my greatest disappointments was his inability to teach a class I was supposed to take from him.He was free with his knowledge and a pioneer in glass fusing. He will be missed.
- Mon Oct 31, 2022 11:51 am
- Forum: Techniques and Tools
- Topic: Polishing Question
- Replies: 2
- Views: 4178
Polishing Question
Hi, I am trying to get a clear polish on all sides with a Somaca wet belt sander, I am wondering if I can use cerium oxide with my Cork belt? Can't seem to find a 4x106 felt belt. THANKS
- Tue May 24, 2022 5:32 pm
- Forum: Techniques and Tools
- Topic: Enamel & powder
- Replies: 11
- Views: 31281
Enamel & powder
Can you mix dry enamel with clear powder to make custom colors?
- Thu Sep 16, 2021 5:38 pm
- Forum: Newcomer Forum
- Topic: Smooshing Weights
- Replies: 7
- Views: 48473
Re: Smooshing Weights
Don, if you ha ent used the metal yet, I use kilnsjdlves and other refractory materials to provide the weight
- Thu Sep 16, 2021 5:36 pm
- Forum: Techniques and Tools
- Topic: firepolish for Pressed Glass
- Replies: 2
- Views: 9212
Re: firepolish for Pressed Glass
Thanks Brad
- Thu Sep 16, 2021 5:33 pm
- Forum: Techniques and Tools
- Topic: Silver Fuming
- Replies: 6
- Views: 8955
Re: Silver Fuming
Too many steps then
- Thu Sep 16, 2021 5:32 pm
- Forum: Techniques and Tools
- Topic: Duraboard as elevated second shelf?
- Replies: 4
- Views: 5583
Re: Duraboard as elevated second shelf?
FYI..I routinely fire 2 levels in my kiln I fire to 1385 to tack fuse on the shelf, and use the floor under the shelf to slump, this seems to work well, but there is a good bit of difference in the temp.
- Sat Sep 04, 2021 12:28 pm
- Forum: Techniques and Tools
- Topic: Silver Fuming
- Replies: 6
- Views: 8955
Re: Silver Fuming
While it did react, and there was some Halo, it wasn't nearly as intense as on the glass itself. Tried several different thicknesses of the powder, but it distorted the transparency in relation to its depth. So, these will just cost more in the future. So the answer is Yes, but....
- Fri Sep 03, 2021 6:49 pm
- Forum: Techniques and Tools
- Topic: Silver Fuming
- Replies: 6
- Views: 8955
Re: Silver Fuming
Thanks, I always put the silver on top, I will run a cpl of text tiles tonight.
- Fri Sep 03, 2021 5:42 pm
- Forum: Techniques and Tools
- Topic: Silver Fuming
- Replies: 6
- Views: 8955
Silver Fuming
I have made pieces in the past with Silver foil on BE reactive Ice and gotten a nice fume pattern. I am wondering if I use Tekta and Reactive Ice powder with Silver it will give a similar effect?
- Fri Aug 27, 2021 3:06 pm
- Forum: Techniques and Tools
- Topic: Tiny Hole Saw Bits for a Dremel?
- Replies: 13
- Views: 26647
Re: Tiny Hole Saw Bits for a Dremel?
THK on e bay, wide selection cheap and fairly durable...but lots out there.
- Thu Jun 03, 2021 4:29 pm
- Forum: Techniques and Tools
- Topic: HD Fiber Board
- Replies: 3
- Views: 5911
Re: HD Fiber Board
Contacted Jim, and the other folks you referred me to Brad...working on it. Thanks
- Wed Jun 02, 2021 4:00 pm
- Forum: Techniques and Tools
- Topic: HD Fiber Board
- Replies: 3
- Views: 5911
HD Fiber Board
I need to replace the Fiber Board lid on my Glassglow kiln. It doesn't look too hard, just need to find some materia,l looks as if I need a 30x48" piece 2" thick. It doesn't appear there are any other support for this other than the edges, so rigidity is importa.nt. Suggestions?
- Sat May 15, 2021 2:05 pm
- Forum: Techniques and Tools
- Topic: firepolish for Pressed Glass
- Replies: 2
- Views: 9212
firepolish for Pressed Glass
Hoping that someone can save me some time. Loo king for the lowest temp I can fire 1or 2mm pressed glass to achieve a shiny finish? would a light dusting of clear powder help? trying to avoid any thickening or rolling of the edges Thanks
- Wed Feb 03, 2021 4:19 pm
- Forum: Techniques and Tools
- Topic: Flat Lap
- Replies: 13
- Views: 29698
Re: Flat Lap
Just to update on this Tom immediately, and I after a bit of explanation have both received full refunds..Thank You Paypal.
- Sat Jan 16, 2021 3:25 pm
- Forum: Techniques and Tools
- Topic: Flat Lap
- Replies: 13
- Views: 29698
Re: Flat Lap
Update, I received a. Package from China today that is from who responded to my order. Instead of a Potter's Wheel, I got an imitation Gold ring....whoopee!
- Mon Jan 11, 2021 4:08 pm
- Forum: Techniques and Tools
- Topic: Scrap into sheet?
- Replies: 8
- Views: 15590
Re: Scrap into sheet?
The black seemed to come out fine..I sandblasted both sides and have it in now on thinfire to Firepolish.
- Sat Jan 09, 2021 2:35 pm
- Forum: Techniques and Tools
- Topic: Scrap into sheet?
- Replies: 8
- Views: 15590
Re: Scrap into sheet?
Trying this with Black scrap now..?it's cooling