I am fusing two large sheets of Bullseye White (013-30) together. They are 13" x 29". Do I need to adjust the fusing schedule due to the size?
- Mon Sep 18, 2017 11:05 pm
- Forum: Techniques and Tools
- Topic: Using Bending Glaze
- Replies: 0
- Views: 104543
Using Bending Glaze
I have two tacked pieces that have devit on them. Both have dichro on them. Has anyone used Bending Glaze on dichro? Wondering if I should spray the whole piece and refire at a slumping temp. If not compatible with dichro, would brushing the bending solution on the devitted areas help, or create mor...
- Sat Mar 16, 2013 3:09 pm
- Forum: Techniques and Tools
- Topic: Vitrigraph Kilns
- Replies: 8
- Views: 11469
Vitrigraph Kilns
I am interested in buying a Vitrigraph Kiln. What's the best brand?
- Sun Dec 23, 2012 4:33 pm
- Forum: Techniques and Tools
- Topic: Screen Melts
- Replies: 35
- Views: 39507
Re: Screen Melts
Thanks for the warning. I have tried one screen melt, and it did make a mess in the kiln, but I didn't think about shards of glass getting into the elements. I did find a website for a company called TWP. They sell welded stainless mesh by the square foot. I ordered some and will try to make my own ...
- Sun Dec 23, 2012 12:57 pm
- Forum: Techniques and Tools
- Topic: Screen Melts
- Replies: 35
- Views: 39507
Screen Melts
Can dichro or irid glass be used for a screen melt? Also, where can I buy welded stainless mesh so I can make my own screens?