Re: Sand Mold Basics
I'm joining this thread kind of late but I have a question and I'm hoping one of you might know the answer. I have been told by multiple knowledge glass casters (Norman Courtney is one - he works Bertil Vallien quite often and was my teacher at Pilchuck) that I need a mix of 120 and 180 Olivine for ...