by Dairy Queen
Tue Aug 07, 2012 9:34 am
Forum: Techniques and Tools
Topic: how to create a flat bottom on the slump with a ball mould?
Replies: 22
Views: 12188

Re: how to create a flat bottom on the slump with a ball mou

I'd mix up a very thin, self leveling plaster mold mix. Pour to depth desired. Probably need no more than 1/2 cup. I have and love that mold. Balance is forced upon your piece by this mold. But I can understand your love of the shape, and need for stability.
by Dairy Queen
Wed Jul 25, 2012 9:35 am
Forum: Techniques and Tools
Topic: rust on glass from reciprolap
Replies: 14
Views: 7668

Re: rust on glass from reciprolap

ps. I searched the archives, but found only 3 mentions of reciprolap (the way I spell it) and no mentions of rust.
by Dairy Queen
Wed Jul 25, 2012 9:34 am
Forum: Techniques and Tools
Topic: rust on glass from reciprolap
Replies: 14
Views: 7668

rust on glass from reciprolap

I recently purchased a reciprolap, which I LOVE! Problem: rust on glass, how to remove It came covered in dark oil. Once the oil was removed from repeated usage, the plate began to rust. I was left with rust stains on opaque glasses. So, I re-oiled the plate with motor oil. It works fine now, but ho...
by Dairy Queen
Fri Jun 29, 2012 9:25 pm
Forum: Photos and Stuff
Topic: Technique: Simple Lay Up Gives Depth
Replies: 7
Views: 4734

Re: Technique: Simple Lay Up Gives Depth

Marty, Many Warm Glass readers have followed me on Facebook, and requested I post techniques on Warm Glass. They have never seen simple layering before. I am not posting for the old dog, or the fossils. I will never do anything to impress the old guard. I am posting for new folks, who have never hea...
by Dairy Queen
Fri Jun 29, 2012 7:52 pm
Forum: Techniques and Tools
Topic: Graphics
Replies: 23
Views: 15004

Re: Graphics

Why are these photos appropriate for techniques, but mine are not? Brad Walker's expressed reason for moving my technique photos applies to this thread, as well: Because the Photos and Stuff folder is where you share photos of your work. If this had been a photo of a novel technique or something rea...
by Dairy Queen
Fri Jun 29, 2012 9:19 am
Forum: Photos and Stuff
Topic: Technique: Simple Lay Up Gives Depth
Replies: 7
Views: 4734

Re: Technique: Simple Lay Up Gives Depth

Why has this posting been moved to photographs? It directly depicts a TECHNIQUE that I would like to share.
by Dairy Queen
Fri Jun 29, 2012 7:15 am
Forum: Photos and Stuff
Topic: Technique: Simple Lay Up Gives Depth
Replies: 7
Views: 4734

Technique: Simple Lay Up Gives Depth

This TECHNIQUE gives lots of DEPTH
(and it should be left in TECHNIQUES and not moved to photos)
There are a few tiny bubbles in the piece after the first firing. To eliminate bubbles entirely, use a chad.
by Dairy Queen
Fri Jun 29, 2012 7:07 am
Forum: Photos and Stuff
Topic: Simple lay up gives depth
Replies: 4
Views: 4032

Re: Simple lay up gives depth

Here is the piece after the first firing. There are some tiny bubbles... Should have used a chad.
by Dairy Queen
Sun Jun 24, 2012 9:06 am
Forum: Photos and Stuff
Topic: Simple lay up gives depth
Replies: 4
Views: 4032

Re: Simple lay up gives depth

Fired results will be out of the kiln on Wed or Thur.
by Dairy Queen
Sat Jun 23, 2012 8:52 am
Forum: Photos and Stuff
Topic: Simple lay up gives depth
Replies: 4
Views: 4032

Re: Simple lay up gives depth

The photo didn't post.

This simple lay up gives much depth to this piece. There will forever be a space between the top and bottom layers. The orange pieces will forever cast a shadow on the stringers below.
by Dairy Queen
Sat Jun 23, 2012 8:46 am
Forum: Photos and Stuff
Topic: Simple lay up gives depth
Replies: 4
Views: 4032

Simple lay up gives depth

This simple lay up gives depth to this piece. There will always be space between the top and bottom layers. Image