by AJK25
Mon Nov 02, 2015 5:00 pm
Forum: Techniques and Tools
Topic: bubbles
Replies: 10
Views: 9228

Re: bubbles

I am so incredibly sorry for not responding. In the past, whenever somebody responded to me, it sent me an email telling me so. And i didnt receive any emails this time, so I assumed that nobody responded. I just logged on to warmglass.com today just to make sure, and i saw everybody's responses. Th...
by AJK25
Thu Oct 29, 2015 10:34 am
Forum: Techniques and Tools
Topic: bubbles
Replies: 10
Views: 9228

bubbles

I am getting bubbles between layers of glass when I fuse Bullseye glass. I have tried a "bubble squeeze," but it hasnt helped. Just wondering if anybody has any thoughts or suggestions. I am fusing 3 layers of glass -- Bullseye Clear Reed on top, and then either aqua tint, white or black a...
by AJK25
Mon Jul 06, 2015 2:26 pm
Forum: Techniques and Tools
Topic: glue
Replies: 6
Views: 4938

glue

Curious if anybody knows of a glue that adheres glass to metal that they think is terrific. I've been using a few glues that are pretty good, but looking for one that is unbelievably good.

Thanks,
Drew Kates
by AJK25
Mon Dec 29, 2014 2:47 pm
Forum: Techniques and Tools
Topic: Spray A
Replies: 11
Views: 6151

Re: Spray A

thanks valerie. I may not be applying it correctly. Perhaps i should look into a mouth atomizer.
by AJK25
Mon Dec 29, 2014 12:24 pm
Forum: Techniques and Tools
Topic: Spray A
Replies: 11
Views: 6151

Re: Spray A

thanks very much. I tried the Spray A and it really didnt work well for me.
by AJK25
Mon Dec 22, 2014 3:17 pm
Forum: Techniques and Tools
Topic: Spray A
Replies: 11
Views: 6151

Re: Spray A

thanks bert
by AJK25
Mon Dec 22, 2014 2:05 pm
Forum: Techniques and Tools
Topic: Spray A
Replies: 11
Views: 6151

Re: Spray A

Thanks so much. I fired at full temperature. I think i may have applied too much Spray A. I think spraying it on will be a better choice than brushing it on.
by AJK25
Mon Dec 22, 2014 11:47 am
Forum: Techniques and Tools
Topic: Spray A
Replies: 11
Views: 6151

Spray A

I am having some devitrification problems when i fire Bullseye cobalt blue glass. I purchased Spray A, and applied it will a brush, but it left some white streaks after firing. I'm trying to find the best way to apply the Spray A. I'm thinking that perhaps i should spray it on, rather than brush it ...
by AJK25
Wed Jul 30, 2014 10:35 am
Forum: Techniques and Tools
Topic: kiln wash sticking
Replies: 4
Views: 3110

Re: kiln wash sticking

thanks
by AJK25
Mon Jul 28, 2014 12:58 pm
Forum: Techniques and Tools
Topic: kiln wash sticking
Replies: 4
Views: 3110

Re: kiln wash sticking

i think the thermocouple is ok. Might be the kiln wash.

Thanks Marty.
by AJK25
Mon Jul 28, 2014 11:36 am
Forum: Techniques and Tools
Topic: kiln wash sticking
Replies: 4
Views: 3110

kiln wash sticking

All of a sudden my kiln wash is sticking to my pieces of fused glass. Not sure why. I've been using the same kiln boards and kiln wash for years, and it never used to stick. Now it's sticking. Not sure why. Could it be because the boards are getting older? I'm using the same kiln wash (from Bullseye...
by AJK25
Wed Jun 11, 2014 10:12 am
Forum: Techniques and Tools
Topic: glass breaking
Replies: 3
Views: 2745

Re: glass breaking

thanks for your suggestions, Warren and Rosanna. I appreciate it.
by AJK25
Tue Jun 10, 2014 6:27 pm
Forum: Techniques and Tools
Topic: glass breaking
Replies: 3
Views: 2745

glass breaking

i have been fusing small pieces of glass for many years now (1.25" square, between 3 and 5 layers of 3mm Bullseye fusible glass). I've had no problems until recently. Some of my glass has started to break off, and i'm not sure why. Somebody told me that it may be because of the thickness of my ...
by AJK25
Mon Mar 10, 2014 9:44 am
Forum: Techniques and Tools
Topic: firing problem
Replies: 23
Views: 11392

Re: firing problem

i purchased it from the manufacturer
by AJK25
Tue Mar 04, 2014 4:10 pm
Forum: Techniques and Tools
Topic: firing problem
Replies: 23
Views: 11392

Re: firing problem

yes, the elements are glaring red. My kiln repairman is coming by tomorrow. He has already checked to make sure it's pulling the correct amps, and it is. He is checking the volts tomorrow. Is there anything else to check while he's here? I chatted with Bert Weiss, and he feels that if it is pulling ...
by AJK25
Tue Mar 04, 2014 3:40 pm
Forum: Techniques and Tools
Topic: firing problem
Replies: 23
Views: 11392

Re: firing problem

it has a more powerful element and is still acting this way.
by AJK25
Tue Mar 04, 2014 11:31 am
Forum: Techniques and Tools
Topic: firing problem
Replies: 23
Views: 11392

Re: firing problem

thanks for all of the replies. Regarding electrical issues (Bert), the kiln is pulling 29 amps, and is 24" x 24" x 12" (interior).
by AJK25
Mon Mar 03, 2014 7:05 pm
Forum: Techniques and Tools
Topic: firing problem
Replies: 23
Views: 11392

Re: firing problem

yes, i was told it would work with 208 elements.

i'm ok with putting in the fiber board, as long as it works.
by AJK25
Mon Mar 03, 2014 5:35 pm
Forum: Techniques and Tools
Topic: firing problem
Replies: 23
Views: 11392

firing problem

I have a Glassglow Model 300 kiln.It has worked beautifully for me for 8 years, so I bought another one, and I am having some issues with the new one. The builder of the kiln told me it may have something to do with the fact that different bricks were used for this new kiln (because the manufacturer...

Go to advanced search

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com