by dawnsud
Sat Aug 25, 2012 11:15 am
Forum: Techniques and Tools
Topic: Clearance between mold and kiln wall
Replies: 4
Views: 2038

Re: Clearance between mold and kiln wall

Good point, Bert.
by dawnsud
Fri Aug 24, 2012 1:35 pm
Forum: Techniques and Tools
Topic: Clearance between mold and kiln wall
Replies: 4
Views: 2038

Re: Clearance between mold and kiln wall

I chickened out and am using the big kiln. Rosanna, your warning about the temp was right on. The piece has 2 layers of small squares mixed between larger solid pieces and that has a tendency to crack on the slump. Plus it is a brand new mold and I'd hate to lose it on the first firing. Thanks for t...
by dawnsud
Wed Aug 22, 2012 9:55 pm
Forum: Techniques and Tools
Topic: Clearance between mold and kiln wall
Replies: 4
Views: 2038

Clearance between mold and kiln wall

I want to do a slump into a ceramic mold. There is only 1/8" clearance between the corners of the mold and the walls of the kiln. The elements are only on the top, not the sides. Am I asking for trouble if I try this?
by dawnsud
Fri Aug 10, 2012 3:28 pm
Forum: Techniques and Tools
Topic: kilns and storms--power surges?
Replies: 9
Views: 5871

Re: kilns and storms--power surges?

After a power surge turned on my Evenheat kiln when I was gone, I've stopped leaving it plugged in. Another time, a surge caused it to lose the Seg 0 info which stops it. It ran away to about 1700 degrees before I unplugged it. It has an old Rampmaster controller. Newer kiln from Skutt is supposed t...
by dawnsud
Wed Aug 01, 2012 4:00 pm
Forum: Techniques and Tools
Topic: how to remove silicone glue?
Replies: 9
Views: 5726

Re: how to remove silicone glue?

Paint thinner works on E6000. Might try it on silicone.
by dawnsud
Fri Jul 20, 2012 10:42 pm
Forum: Photos and Stuff
Topic: Finally some new images from my Tropical Woman series
Replies: 27
Views: 18672

Re: Finally some new images from my Tropical Woman series

Your talent just amazes me. These are stunning. Let us know when you show these because there will be a lot of interest.
by dawnsud
Fri Jul 20, 2012 11:38 am
Forum: Techniques and Tools
Topic: Uneven bowl slumping
Replies: 17
Views: 12539

Re: Uneven bowl slumping

You said you checked the mold and the shelf and found them to be level. Did you use a level on top of the glass after you put it in the mold?
by dawnsud
Fri Jul 20, 2012 11:36 am
Forum: Techniques and Tools
Topic: Dichro Slide
Replies: 7
Views: 3873

Re: Dichro Slide

Most of the manufacturers have very helpful tech support people. If you don't know the manufacturer, call your supplier and find out.
by dawnsud
Wed Jul 18, 2012 1:46 pm
Forum: Photos and Stuff
Topic: a table
Replies: 24
Views: 14556

Re: a table

Both pieces are stunning, Nina. I love the combination of wood and glass because of the contrast. I love, love, love the sculpture Life of Trees. Hope it sells for you. I'd love to see it in a public setting where many people can enjoy it.
by dawnsud
Wed Jul 11, 2012 1:38 pm
Forum: Jewelry Making
Topic: Donut Bails
Replies: 4
Views: 5288

Re: Donut Bails

The bails will work well. Thanks for the recommendation.
by dawnsud
Wed Jul 11, 2012 1:37 pm
Forum: Jewelry Making
Topic: Donut Bails
Replies: 4
Views: 5288

Re: Donut Bails

The only ones that are $10 are the small geometric pendants that I sell to girls under the age of 14. It often leads to other sales from the Mom. I am getting most this size done in 1 firing. I use a 1/2 inch wide painter's brush to flatten the top. Then I use a very small, angled painter's brush an...
by dawnsud
Tue Jul 10, 2012 8:40 pm
Forum: Techniques and Tools
Topic: Go and stop and go? Or just go?
Replies: 30
Views: 15858

Re: Go and stop and go? Or just go?

More holds====more wear on the controller and relays===more replacement, maintenance? Just a suspicious person.
by dawnsud
Tue Jul 10, 2012 11:09 am
Forum: Jewelry Making
Topic: Donut Bails
Replies: 4
Views: 5288

Donut Bails

I'm selling lots of the pendants made with Colour de Verre molds--easy to make, fun to experiment with color combos, priced from $10 to $20 with satin cord. I want to attach some of the pillow pendant pieces to beaded necklaces. I hate wire wrapping. So I wanted to use a donut bail to attach them. I...
by dawnsud
Sun Jul 01, 2012 10:12 am
Forum: Photos and Stuff
Topic: Chasing the Eclipse
Replies: 15
Views: 9489

Re: Chasing the Eclipse

You are doing some amazing things and creating art, instead of just technique. You received compliments from some outstanding glass artists. Be happy!
by dawnsud
Sun Jul 01, 2012 10:10 am
Forum: Photos and Stuff
Topic: Frit Painting
Replies: 6
Views: 5622

Re: Frit Painting

Awesome. You capture the spirit of the place.
by dawnsud
Tue Jun 19, 2012 12:56 pm
Forum: Photos and Stuff
Topic: Brave Reasons
Replies: 17
Views: 9917

Re: Brave Reasons

Stunning and original as always with your work.
by dawnsud
Tue Jun 05, 2012 5:30 pm
Forum: Techniques and Tools
Topic: Touch sensitive glass
Replies: 6
Views: 4800

Re: Touch sensitive glass

Kevin, thanks for the posting on this amazing glass.
by dawnsud
Mon Jun 04, 2012 10:01 am
Forum: Newcomer Forum
Topic: cutting circles
Replies: 14
Views: 9075

Re: cutting circles

There is a video of Patty Gray cutting circles on the Spectrum website. It is very well done.
by dawnsud
Fri Jan 18, 2008 5:55 pm
Forum: Techniques and Tools
Topic: SS mold
Replies: 0
Views: 2962

Re: SS mold

I tried them all. Now I use a brush and a 1875 watt hairdryer. Worked better than my husband's heat gun even.
by dawnsud
Thu Jan 10, 2008 5:40 pm
Forum: Photos and Stuff
Topic: 2008 experiment No. 1
Replies: 0
Views: 4477

Re: 2008 experiment No. 1

Thanks for sharing. You've given me a great idea for my test strips from my weaving pieces. Fun to see.

Go to advanced search

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com