by lorimendenhall
Thu Dec 19, 2013 10:53 am
Forum: Business Topics
Topic: Indiegogo?
Replies: 11
Views: 7865

Re: Indiegogo?

why not just ask the parents to donate some money for each child who participates? it would not be mandatory but I am sure the majority of parents would pay. it would not have to be a lot, maybe $10, or whatever. I was very involved in my kids' elementary school and the moms would have been glad to ...
by lorimendenhall
Wed Dec 18, 2013 2:05 pm
Forum: Newcomer Forum
Topic: Help putting frit in mold
Replies: 5
Views: 4172

Re: Help putting frit in mold

if it's a mold you are working upside down. depending on the look you want you could approach it different ways. when I make molded dragonflies I strategically place the dichro pieces where I want them and then fill up with non-dichro frit. if the dichro frit you're using is clear then I think mixin...
by lorimendenhall
Tue Dec 17, 2013 12:31 pm
Forum: Newcomer Forum
Topic: big bubble at base of bowl
Replies: 9
Views: 6754

Re: big bubble at base of bowl

that's my problem - I forgot to pray to the kiln gods!!!! actually thank you for posting the schedule that worked. it seems very conservative and I plan to try something very similar after I get this bad boy fused flat again.
by lorimendenhall
Sat Dec 14, 2013 8:21 pm
Forum: Newcomer Forum
Topic: big bubble at base of bowl
Replies: 9
Views: 6754

Re: big bubble at base of bowl

re-fuse flat first it is. thanks guys. yes, I am working on why I got the bubble. I think I might have ramped too fast even though it was only 300 dph.
by lorimendenhall
Fri Dec 13, 2013 8:22 pm
Forum: Newcomer Forum
Topic: big bubble at base of bowl
Replies: 9
Views: 6754

big bubble at base of bowl

I have a gorgeous bowl with a big bubble in the center from slumping. do I have to fire it flat and re-slump or can I simply attempt to reslump putting it back into the mold as is? I've been told different things so wonder what the sages here think. thanks so much. ps the bowl is 12" diameter, ...
by lorimendenhall
Thu Dec 12, 2013 2:01 am
Forum: Newcomer Forum
Topic: firing a new mold
Replies: 9
Views: 6149

Re: firing a new mold

this mold is manufactured by Creative Ceramics and I think it was a Bullseye branded item.
by lorimendenhall
Wed Dec 11, 2013 2:33 pm
Forum: Newcomer Forum
Topic: firing a new mold
Replies: 9
Views: 6149

Re: firing a new mold

I've never pre-fired a mold BUT I just got a new one and the instructions say: "pre-firing is recommended for molds larger than 30cm. this process strengthens the inner structures and makes the mold less susceptible to thermal shock." the directions are to go like you say below, 50 degrees...
by lorimendenhall
Wed Dec 11, 2013 2:27 pm
Forum: Newcomer Forum
Topic: Buying first kiln...will specific project fit?
Replies: 8
Views: 4819

Re: Buying first kiln...will specific project fit?

your mold is 14.5 but the shelf is only 14? that sounds like it would be a super tight squeeze and not the best idea. but I don't truly know, just sounds like you're pushing it. I have the 19" clamshell with an 18" shelf and I love it.
by lorimendenhall
Wed Dec 11, 2013 2:25 pm
Forum: Newcomer Forum
Topic: super easy question about priming a mold
Replies: 4
Views: 3117

Re: super easy question about priming a mold

thanks for your reply. I've been doing a few per coating so I guess I'll just keep doing that for now.
by lorimendenhall
Tue Dec 10, 2013 10:48 pm
Forum: Techniques and Tools
Topic: Tempered Glass Shards
Replies: 9
Views: 8422

Re: Tempered Glass Shards

good to know and what gorgeous pieces you made!!!!!
by lorimendenhall
Tue Dec 10, 2013 3:35 pm
Forum: Newcomer Forum
Topic: super easy question about priming a mold
Replies: 4
Views: 3117

super easy question about priming a mold

dumb question but I've heard differing info... how many uses can you get out of a ceramic mold primed with Hotline Primo Primer? thanks!
by lorimendenhall
Tue Dec 10, 2013 2:25 pm
Forum: Techniques and Tools
Topic: Tempered Glass Shards
Replies: 9
Views: 8422

Re: Tempered Glass Shards

I was told you are not supposed to fuse tempered glass.
by lorimendenhall
Fri Nov 22, 2013 11:44 pm
Forum: Techniques and Tools
Topic: Advice on a kiln for fusing 17" bowl?
Replies: 11
Views: 6069

Re: Advice on a kiln for fusing 17" bowl?

I've only used it about 5x so far but it certainly seems to heat evenly.
by lorimendenhall
Fri Nov 22, 2013 2:34 am
Forum: Techniques and Tools
Topic: Advice on a kiln for fusing 17" bowl?
Replies: 11
Views: 6069

Re: Advice on a kiln for fusing 17" bowl?

I got the Paragon-19S delivered for a little bit over $1500. It's a clamshell and can take an 18" square shelf. sounds like it's what you are looking for.
by lorimendenhall
Wed Nov 06, 2013 1:32 pm
Forum: Newcomer Forum
Topic: PC monitor as light box for photos
Replies: 4
Views: 4473

Re: PC monitor as light box for photos

why not get a photo tent with some professional lights? not very expensive and works great.
by lorimendenhall
Mon Nov 04, 2013 3:21 pm
Forum: Newcomer Forum
Topic: Am I heating my dichro for too long?
Replies: 5
Views: 3622

Re: Am I heating my dichro for too long?

I've heated dichro for longer and hotter than that and never had that happen. which brand dichro is it?
by lorimendenhall
Sun Oct 06, 2013 11:20 am
Forum: Newcomer Forum
Topic: haze left after stuck kiln wash is removed
Replies: 8
Views: 5821

Re: haze left after stuck kiln wash is removed

I will definitely try the lower temp and longer hold. if that doesn't work I will just reapply each time. thank you all for your help.
by lorimendenhall
Fri Oct 04, 2013 10:25 pm
Forum: Newcomer Forum
Topic: haze left after stuck kiln wash is removed
Replies: 8
Views: 5821

Re: haze left after stuck kiln wash is removed

still getting this problem. it doesn't happen on the first fire of fresh wash but it does on second firings. I didn't think I had to reapply each time. I am going to 1490 and holding for 16 minutes. I realize that's a lot but my kiln is small and if I don't hold for a long time I don't get a full fu...
by lorimendenhall
Thu Oct 03, 2013 1:00 pm
Forum: Newcomer Forum
Topic: Control bubbles
Replies: 9
Views: 6134

Re: Control bubbles

there is bubble powder but I never tried it.
by lorimendenhall
Sat Sep 28, 2013 2:51 pm
Forum: Techniques and Tools
Topic: workshops in Los Angeles/Ventura County area
Replies: 5
Views: 3680

Re: workshops in Los Angeles/Ventura County area

Pacific Art Glass is the place most often mentioned around here. they have huge kilns and lots of classes. in fact, their open house is coming p Oct. 5-6. I'll be there on the 6th.

Go to advanced search

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com