Search found 240 matches
- Fri Dec 07, 2012 9:10 pm
- Forum: Techniques and Tools
- Topic: Screen printing TPI Question
- Replies: 25
- Views: 25592
Re: Screen printing TPI Question
I do a ton of screen printing. CMC based mediums for screen printing, while they work, are not optimum for screening. These mediums do not hold nearly as much enamel in suspension as pine oil or A-14. Pine oil is a mess to deal with so I only use A-14 (a Thompson product). The results are far superi...
- Thu Dec 06, 2012 9:52 pm
- Forum: Techniques and Tools
- Topic: hmmmm.....cookie press?
- Replies: 3
- Views: 4697
Re: hmmmm.....cookie press?
Have tried similar things. The problem is the liquid squeezes out in the first one or two and then you are left with what approaches cement in the gun.
Barry
Barry
- Sun Dec 02, 2012 9:04 pm
- Forum: Board Help
- Topic: Adding photo to private message
- Replies: 1
- Views: 17428
Adding photo to private message
Brad,
Tried to add a photo attachment to a personal message and got the error massage that the extension jpg was not acceptable.
Any way to add a photo to a personal?
Barry
Tried to add a photo attachment to a personal message and got the error massage that the extension jpg was not acceptable.
Any way to add a photo to a personal?
Barry
- Sun Dec 02, 2012 4:12 pm
- Forum: Photos and Stuff
- Topic: Cave Art
- Replies: 17
- Views: 16725
Re: Cave Art
Hope the small cracks don't cause a problem. Could be that they actually enhance the texture of the artwork. The piece is too beautiful to lose.
Great use of color!
Great use of color!
- Sun Dec 02, 2012 4:08 pm
- Forum: Techniques and Tools
- Topic: Vitrification on Opal?
- Replies: 3
- Views: 5192
Re: Vitrification on Opal?
I thought I would put this in this thread. In your case, it sounds like you are just cutting and it really doesn't apply in that case, but here it is anyway. There is a huge difference between "devit" on the top (flat) surface, and the "devit" on the sides of the piece occurring ...
- Fri Nov 30, 2012 1:44 pm
- Forum: Photos and Stuff
- Topic: New Bowl
- Replies: 9
- Views: 10147
Re: New Bowl
I like the design and colors,
Don't be shy about posting. Your work is excellent.
Barry
Don't be shy about posting. Your work is excellent.
Barry
- Thu Nov 29, 2012 11:51 am
- Forum: Techniques and Tools
- Topic: lettering fused into or onto glass
- Replies: 47
- Views: 51502
Re: lettering fused into or onto glass
We do lots of screen printing, which would work for this project. But, it is time consuming to make a screen for each name. A far simpler and effective method of doing this is to go to Office Depot or similar store and buy the sets of vinyl letters. Lots of sizes and fonts. If your budget allows, yo...
- Wed Nov 28, 2012 1:04 pm
- Forum: Photos and Stuff
- Topic: Quiet Sunset
- Replies: 14
- Views: 14719
Re: Quiet Sunset
Glad you shared it!!
Awesome
Barry
Awesome
Barry
- Fri Nov 02, 2012 7:47 pm
- Forum: Techniques and Tools
- Topic: Expandable drums
- Replies: 17
- Views: 22539
Re: Expandable drums
HI Bob,
Just got back into town, so late to this party
I made mine with an arbor from Lortone (about $400) and a local motor from a motor shop($85).
very easy to do.
Drums and wheels added about 250.
Barry
Just got back into town, so late to this party
I made mine with an arbor from Lortone (about $400) and a local motor from a motor shop($85).
very easy to do.
Drums and wheels added about 250.
Barry
- Tue Oct 09, 2012 2:08 pm
- Forum: Techniques and Tools
- Topic: LIQUID GLASS................CMC.............Alternatives
- Replies: 31
- Views: 35683
Re: LIQUID GLASS................CMC.............Alternatives
Jerry,
As a sub for the Flexiglass, try any polyvinyl acetate or Poly-ox based glue such as Elmers, Alenes or Bordens. Mix with a little water to thin some. Use good quality wax paper or treated (for release) aluminum foil. Works quite well.
Barry
As a sub for the Flexiglass, try any polyvinyl acetate or Poly-ox based glue such as Elmers, Alenes or Bordens. Mix with a little water to thin some. Use good quality wax paper or treated (for release) aluminum foil. Works quite well.
Barry
- Thu Oct 04, 2012 4:47 pm
- Forum: Business Topics
- Topic: First Gallery Opening
- Replies: 8
- Views: 11291
Re: First Gallery Opening
yes Risa,
Relax and enjoy it.
Also go to bbakerinc.com and buy his booth design and Sales CDs. You don't need the jury CD for your situation.
Bruce Baker is the king of common sense when it comes to selling arts and crafts.
Barry
Relax and enjoy it.
Also go to bbakerinc.com and buy his booth design and Sales CDs. You don't need the jury CD for your situation.
Bruce Baker is the king of common sense when it comes to selling arts and crafts.
Barry
- Sun Sep 23, 2012 7:56 pm
- Forum: Photos and Stuff
- Topic: Fused glass and 3D printing
- Replies: 8
- Views: 10116
Re: Fused glass and 3D printing
Very Very cool,
Barry
Barry
- Sun Sep 23, 2012 7:53 pm
- Forum: Techniques and Tools
- Topic: Schedule needed for glass nuggets
- Replies: 7
- Views: 9315
Re: Schedule needed for glass nuggets
Vicki,
You may need to hold some at 1450.
Check to see if they are done, then turn off the kiln.
Barry
You may need to hold some at 1450.
Check to see if they are done, then turn off the kiln.
Barry
- Thu Sep 20, 2012 8:09 pm
- Forum: Photos and Stuff
- Topic: Koi
- Replies: 4
- Views: 5825
Re: Koi
Darn it Valerie,
You keep changing on me. The piece is beautiful, and far different from much of your other work. You keep evolving and consistently for the better
Barry
You keep changing on me. The piece is beautiful, and far different from much of your other work. You keep evolving and consistently for the better
Barry
- Sun Sep 16, 2012 12:41 pm
- Forum: Techniques and Tools
- Topic: Has anyone used fusion pens from Fusion headquarters?
- Replies: 2
- Views: 4266
Re: Has anyone used fusion pens from Fusion headquarters?
Try the pilot silver markers...available at Staples (for some reason not available at Office Depot).
Inexpensive and they do withstand firing.
Barry
Inexpensive and they do withstand firing.
Barry
- Fri Sep 14, 2012 11:54 am
- Forum: Jewelry Making
- Topic: making consistant small oval cabs
- Replies: 7
- Views: 12810
Re: making consistant small oval cabs
Another method is to fuse to approximate size and then grind to size and shape. We have a 6 wheel rotary grinder which makes short work of this process.
Barry
Barry
- Sat Sep 08, 2012 10:11 am
- Forum: Photos and Stuff
- Topic: All "eyes" on my website
- Replies: 3
- Views: 5194
Re: All "eyes" on my website
I have watched your are evolve ever since I found your web site(long ago).
It continues to change with the times. I can't say that it has gotten better, because it has been perfect ever since the beginning. In my opinion, no one can match your personal adornment pieces.
Barry
It continues to change with the times. I can't say that it has gotten better, because it has been perfect ever since the beginning. In my opinion, no one can match your personal adornment pieces.
Barry
- Fri Sep 07, 2012 5:09 pm
- Forum: Photos and Stuff
- Topic: Almost There
- Replies: 6
- Views: 8177
Re: Almost There
Beautiful and very well done.
Barry
Barry
- Fri Aug 31, 2012 10:05 am
- Forum: Photos and Stuff
- Topic: Sea Urchin
- Replies: 19
- Views: 21709
Re: Sea Urchin
So Cool!!
- Tue Aug 21, 2012 11:39 pm
- Forum: Photos and Stuff
- Topic: Cellular
- Replies: 20
- Views: 23242
Re: Cellular
I guess I could ditto everything posted.
Piece is great
Barry
Piece is great
Barry