Search found 23 matches
- Tue Dec 30, 2014 5:41 pm
- Forum: Newcomer Forum
- Topic: large piece glass cracking issue
- Replies: 11
- Views: 17538
Re: large piece glass cracking issue
the piece is only 6mm
- Tue Dec 30, 2014 4:26 pm
- Forum: Newcomer Forum
- Topic: large piece glass cracking issue
- Replies: 11
- Views: 17538
Re: large piece glass cracking issue
Thanks for the help. I thought the bullseye glass was both 96coe and compatible, learning curve :) I have only used the spectrum glass pebbles and have not had a problem. I do think the shape was a major contributor. I have attached a pic of a different piece that I did and also slumped it and no pr...
- Tue Dec 30, 2014 2:16 pm
- Forum: Newcomer Forum
- Topic: large piece glass cracking issue
- Replies: 11
- Views: 17538
large piece glass cracking issue
I need some advice. I fired this, and before it was done I turned it off , I think too soon. I turned it back on but too late. It cracked really bad. (Like the days when you boiled a marble and put it in cold water to make it crack on purpose.) Anyway, I re-fired it the next day, but this time I did...