Search found 167 matches
- Mon Oct 27, 2003 9:37 pm
- Forum: Kiln Casting
- Topic: air bubbles in mold material
- Replies: 7
- Views: 9252
air bubbles in mold material
i saw and felt some tiny bumps on a pices of cast glass, and was wondering, are these caused from tiny air bubbles in the mold material,,,,,,,,,is is possible to coat the wax model, or whatever the master that is to be cast, with the BE KILN WASH to give it a BUBBLE FREE BARRIER between the master a...
- Tue Oct 21, 2003 12:20 pm
- Forum: Photos and Stuff
- Topic: New Stuff
- Replies: 16
- Views: 17060
- Tue Oct 07, 2003 10:48 am
- Forum: Business Topics
- Topic: What is your favorite webpage building program?
- Replies: 6
- Views: 7458
the only program that ive used is FRONTPAGE 2000,,,,,microsoft extensions are on, probably all of the host sites, and its an easy program for me to use,,,i use about 1% of the features, since i have a very basic site, which i use for pic hosting, the other programs i cant say, but i can say this, if...
- Mon Oct 06, 2003 4:57 pm
- Forum: Techniques and Tools
- Topic: fusing with fiberboard to make holes
- Replies: 19
- Views: 17095
- Sun Oct 05, 2003 10:27 am
- Forum: Techniques and Tools
- Topic: What is a powder wafer?
- Replies: 31
- Views: 35659
- Sat Oct 04, 2003 10:48 am
- Forum: Techniques and Tools
- Topic: hey bert
- Replies: 4
- Views: 5175
what did the master glass cutter do,,,using his palm and all,,, ive tried cutting glass right out to the kiln, when still hot, and that seems to work, but one thing im having problems with, when i put the plyers on the glass, the glass tends to crumble, even if its cold, when trying to break the gla...
- Fri Oct 03, 2003 10:32 pm
- Forum: Techniques and Tools
- Topic: hey bert
- Replies: 4
- Views: 5175
hey bert
hey there,,what is this SCORE AND TORCH thing,,,,,thanks, rodney
- Tue Sep 30, 2003 12:36 am
- Forum: Photos and Stuff
- Topic: A retro piece for the older folks
- Replies: 15
- Views: 17080
- Wed Sep 24, 2003 6:38 pm
- Forum: Business Topics
- Topic: Getting OUT Of A Gallery
- Replies: 17
- Views: 23974
- Wed Sep 24, 2003 6:21 pm
- Forum: Techniques and Tools
- Topic: Should I buy a Skutt kiln or JenKen???? Tell me why?
- Replies: 10
- Views: 12379
- Mon Sep 22, 2003 11:06 am
- Forum: Techniques and Tools
- Topic: Permanent nose butter and check fixing
- Replies: 8
- Views: 8141
Re: Permanent nose butter and check fixing
then rubbing it on with a rag. Clean up with pure acetone. Throw away the rags when you're done. It can leave a very subtle pattern from the wiping but you have to look very hard to see it. As always, glue in well ventilated places, try to keep your skin away from epoxy and acetone and test these t...
- Tue Sep 16, 2003 9:32 pm
- Forum: Techniques and Tools
- Topic: Thompson Enamels
- Replies: 3
- Views: 3557
- Tue Sep 16, 2003 2:08 am
- Forum: Techniques and Tools
- Topic: POWDERED FRIT,,,,,,,ENAMAL ?
- Replies: 1
- Views: 2678
POWDERED FRIT,,,,,,,ENAMAL ?
im wondering about the fine powder that is left over after the crushing process to make frit,,,,,,,,,,,,,,,,,im lead to believe that this powder, if put into a thick piece for pate de verre, in volume, will make for a cloudy appearence, but is this the stuff that people use for enamalling,,,where on...
- Wed Aug 20, 2003 11:05 am
- Forum: Business Topics
- Topic: Carpet
- Replies: 4
- Views: 6600
- Tue Aug 19, 2003 11:29 pm
- Forum: Techniques and Tools
- Topic: dichro strategy
- Replies: 9
- Views: 8641
when you get those little BURRS, on the surface from the dichro,,,,you should be able to just hit it lightly ( by hand ) with a piece of 120 grit sand paper, and not even worry about refiring, this works to make the surface smooth enough to avoid snags, but it just depends on what you want for a fin...
- Tue Aug 19, 2003 9:50 am
- Forum: Techniques and Tools
- Topic: PATTERN BAR,,,,,,BREAKING
- Replies: 5
- Views: 5644
- Sun Aug 17, 2003 1:58 pm
- Forum: Techniques and Tools
- Topic: color combos
- Replies: 4
- Views: 5010
Re: color combos
[quote="ellen abbott"]even at frit size 1 is so dense that when held up to the light it becomes very spotty. Every grain of the lt pink is discernable, no matter the ratio or other colors in the mix. Any suggestions? if the frit is visable on the surface, as flecks, it seems that they woul...
- Sun Aug 17, 2003 1:43 pm
- Forum: Techniques and Tools
- Topic: color combos
- Replies: 4
- Views: 5010
- Sun Aug 17, 2003 4:43 am
- Forum: Techniques and Tools
- Topic: PATTERN BAR,,,,,,BREAKING
- Replies: 5
- Views: 5644
PATTERN BAR,,,,,,BREAKING
i remember seeing something where a guy has this pattern bar over a sharp edge, and then whacks the thing, and that breaks off a piece of the bar,,,,has anyone done this,,,,the specifics would be appreciated,,,im trying to find out a way of making slices, WITHOUT a saw,,,,,,can someone tell me how l...
- Sat Aug 16, 2003 12:28 pm
- Forum: Techniques and Tools
- Topic: BORAX Qs,,,,,sprayer,,,recipe
- Replies: 3
- Views: 4247
BORAX Qs,,,,,sprayer,,,recipe
does anyone have a suggestion for a spayer that wont get clogged with borax,,,,,,,,,also is there there a PERFECT mixture for the borax, is more better, is less better,,,,thanks,rodney