Search found 114 matches
- Tue Apr 25, 2017 8:57 am
- Forum: Newcomer Forum
- Topic: Car window glass
- Replies: 3
- Views: 8668
Car window glass
Hello ! Please can anybody give me a schedule for firing and slumping a bowl of Car window Glass (I hope I use the right words in English for this material ) Thank you, Jan from Holland
- Wed Oct 19, 2016 7:56 am
- Forum: Newcomer Forum
- Topic: Silver Sand for Sandmold
- Replies: 4
- Views: 8529
Re: Silver Sand for Sandmold
Yes, now I understand the problem: did translate the Dutch word, but now I realise it is bad translation :) Zilverzand (Dutch) = Quartz sand , silica sand or white sand is fine-grained, white, extremely pure sand with low iron content . It consists almost entirely of quartz (SiO 2 ) Now I know it is...
- Tue Oct 18, 2016 8:24 am
- Forum: Newcomer Forum
- Topic: Silver Sand for Sandmold
- Replies: 4
- Views: 8529
Re: Silver Sand for Sandmold
Difficult question, or did I give to little information ? greetings from Holland, Jan
- Wed Oct 12, 2016 7:52 am
- Forum: Newcomer Forum
- Topic: Silver Sand for Sandmold
- Replies: 4
- Views: 8529
Silver Sand for Sandmold
Hello ! Is it possible to use Silver Sand for making a Sandmold (sand and Aluminium Hydrate) ? Jan
- Thu Nov 12, 2015 9:43 am
- Forum: Newcomer Forum
- Topic: "Pebbles"....making yourself ?
- Replies: 5
- Views: 11801
Re: "Pebbles"....making yourself ?
Hello, the link is not working anymore ?? Not so clever, forgot to archive the schedule. JanJenna wrote:"Pebbles" are also called nuggets. Here is link to a previous post about making them...
http://www.warmglass.com/phpBB/viewtopi ... ts#p240202
- Tue Oct 20, 2015 7:18 am
- Forum: Newcomer Forum
- Topic: Curious to know !
- Replies: 7
- Views: 13222
Re: Curious to know !
Thank you all for your answers ! Buying Graham stone's book is perhaps not so expensive as I thought earlier (loosing glass etc.) Jan de Jong
- Mon Oct 12, 2015 12:52 pm
- Forum: Newcomer Forum
- Topic: Curious to know !
- Replies: 7
- Views: 13222
Re: Curious to know !
@Kevin: Thank you for your answer ! As for the book: Great, but for the few pieces I fire in a year (hobby !) I use the firing schedules from Spectrum. For the first time I did fire a 1 1/2 inch thick piece and did note the wrong things on a piece of paper to set the schedule. Stupid! So, this has h...
- Mon Oct 12, 2015 6:15 am
- Forum: Newcomer Forum
- Topic: Curious to know !
- Replies: 7
- Views: 13222
Curious to know !
Hello ! Did write wrong the firing-schedule of a 37 1/2 cm (1 1/2 inch) thick piece of Spectrum96 on a note for by the kill. The good Step 4 was afap and hold 3 hrs. Now I did fire with this Step 4: 750 C. (1382 F.) to 510 C. (950 F.) and No hold. The piece was broken ! Stupid mistake of course, but...
- Fri Sep 04, 2015 9:13 am
- Forum: Newcomer Forum
- Topic: Pre-firing Stringers
- Replies: 6
- Views: 13325
Re: Pre-firing Stringers
Okay.....thank you all for your respons ! greetings from Holland, Jan de Jong
- Sun Aug 30, 2015 7:51 am
- Forum: Newcomer Forum
- Topic: Pre-firing Stringers
- Replies: 6
- Views: 13325
Re: Pre-firing Stringers
@ Steven Richard: Thank you for your answer, but is there a simple, quick firing-schedule known for this stringers ?? I have to do much stringers, so my choice is pre-firing. greetings from Holland, Jan
- Sun Aug 30, 2015 5:14 am
- Forum: Newcomer Forum
- Topic: Pre-firing Stringers
- Replies: 6
- Views: 13325
Pre-firing Stringers
Hello ! I wonder which simple quick schedule I can use to pre-fire Stringers to avoid rolling ? Jan de Jong
- Sun Aug 30, 2015 5:08 am
- Forum: Newcomer Forum
- Topic: Plate of 4 layers
- Replies: 3
- Views: 7874
Re: Plate of 4 layers
My client (my cousin) desided to choose for tackfuse. With this as result:
http://jandejong-glas.nl/?page_id=1393 Thank you for your help ! Jan de Jong (Holland)
http://jandejong-glas.nl/?page_id=1393 Thank you for your help ! Jan de Jong (Holland)
- Sun Aug 23, 2015 9:09 am
- Forum: Newcomer Forum
- Topic: Plate of 4 layers
- Replies: 3
- Views: 7874
Plate of 4 layers
Hello ! Has been asked to make a plate for a wedding. The measurement: about 28 x 28 cm. I have already fired the background of 2 layers and now I must apply the wedding couple ......containing 2 layers.... so total 4 layers. Normally I fire the 3rd and 4th layer with a "contour" fuse, but...
- Sun May 10, 2015 9:12 am
- Forum: Newcomer Forum
- Topic: Making your own..... shards
- Replies: 10
- Views: 16738
Re: Making your own..... shards
@ Jerry: The translation site is not so good, but I did understand what you mean ! Thank you !
Someone who did try firing on wires ? Jan
Someone who did try firing on wires ? Jan
- Sat May 09, 2015 9:59 am
- Forum: Newcomer Forum
- Topic: Making your own..... shards
- Replies: 10
- Views: 16738
Re: Making your own..... shards
I don't understand the question :?: Brad Walker writes in his book about this ! Making your own "shards". Possible via a drop (and a square is to prefer) and making a square (RVS) with nichrome wire on it. Sorry, my knowledge of the English language is too poor to explain it on the right ...
- Sat May 09, 2015 6:58 am
- Forum: Newcomer Forum
- Topic: Making your own..... shards
- Replies: 10
- Views: 16738
Making your own..... shards
Hello! I read about this in the Warmglass book and here on this site.
I wonder what is the best method: Drop square, or a square with wire on it (and what is then the best amount between the wires ??) ??
Thank you for your help ! Jan de Jong
I wonder what is the best method: Drop square, or a square with wire on it (and what is then the best amount between the wires ??) ??
Thank you for your help ! Jan de Jong
- Mon Feb 02, 2015 11:54 am
- Forum: Newcomer Forum
- Topic: "Pebbles"....making yourself ?
- Replies: 5
- Views: 11801
Re: "Pebbles"....making yourself ?
Thank you Jenna ! I did not know they were called nuggets too Jan de Jong
- Mon Feb 02, 2015 8:40 am
- Forum: Newcomer Forum
- Topic: "Pebbles"....making yourself ?
- Replies: 5
- Views: 11801
"Pebbles"....making yourself ?
Hello ! Is it possible to make "Pebbles" yourself ? If yes....different diameters ? Thank you for your help ! Jan
- Tue Jan 06, 2015 8:39 am
- Forum: Newcomer Forum
- Topic: 4 Seasons.... Break
- Replies: 12
- Views: 16273
Re: 4 Seasons.... Break
Hello ! I did glue the glass on "Trespa". Now on the surface I still must glue the breaks and I intend to do that with epoxy glue. Now I wonder if it is a good idea (or not !) to put some Powder on this breaks to mask them ??? Will this mask the breaks or just make them worse ? Anybody exp...
- Tue Nov 11, 2014 4:55 pm
- Forum: Newcomer Forum
- Topic: 4 Seasons.... Break
- Replies: 12
- Views: 16273
Re: 4 Seasons.... Break
About point 1: I did contact Bert Weiss and he suggested to fire the UV-glued piece to 200-225 C. with a 15 min. hold. Good chance the glass will be seperated !! Thank you very much Bert !! After cleaning and removing rest of the glue I can refire the piece. I will tackfuse this piece with a (fully...