Shelf Paper
I agree with Jerry......I don't like the smell, the contamination in the kiln and the messy cleanup after using thinfire. Kiln wash may be a little more work but it is my preference.
Don
Don
- Wed Jun 04, 2003 10:00 pm
- Forum: Techniques and Tools
- Topic: What impresses you?
- Replies: 17
- Views: 14731
What impresses me
In short "Concept" and "Execution"
Don
Don
- Tue Jun 03, 2003 11:55 am
- Forum: Techniques and Tools
- Topic: kiln mishap
- Replies: 7
- Views: 8823
Evenheat lid
Deena I don't see how this is causing you such trouble. The chain holding my lid is exactly as you describe and has never been a problem. Could it be your chain is too long thus causing your lid to open too far causing extra pressure on these screws? My chain just allows my lid to slightly go past t...
- Thu May 29, 2003 1:03 pm
- Forum: Techniques and Tools
- Topic: Spectrum blues revisited
- Replies: 17
- Views: 14208
I don't believe the greenish yellow Spectrum had anything to do with envioronmental issues in Washington State. That was just the Reds, Oranges and Caramel colours. I'm glad to hear they are going to change back to a purer yellow. Thanks foe the heads up. I do think they should have been more forthc...
- Thu May 22, 2003 11:25 am
- Forum: Techniques and Tools
- Topic: Iridized Glass? What is it?
- Replies: 6
- Views: 7601
Irid glass
Hi Ron........Your irid surface looks quite smooth(no cracks).
I have blasted a design on "96" black irid, then fired it to polish blasted area. Mine always seem to have cracks in final irid exposed surface.
Fuse at 1450 after blasting, Slump at 1260.
Don
I have blasted a design on "96" black irid, then fired it to polish blasted area. Mine always seem to have cracks in final irid exposed surface.
Fuse at 1450 after blasting, Slump at 1260.
Don
- Tue Apr 22, 2003 11:07 pm
- Forum: Techniques and Tools
- Topic: Mica/Klyr fire problems
- Replies: 2
- Views: 4547
Mica/Klyr fire problems
I'm about ready to give up on mica powders. I air brush on many coats of mica/klyr fire then find it hard to peel off my mask and retain a clean edge. The coating is sealed across the edge causing it to lift. tried running knife along edge after spraying, this helped somewhat but was very time consu...
- Sat Apr 05, 2003 9:45 pm
- Forum: Techniques and Tools
- Topic: Another Kiln Repair Q
- Replies: 15
- Views: 18983
- Mon Mar 31, 2003 11:07 am
- Forum: Techniques and Tools
- Topic: sagging element emergency care?
- Replies: 12
- Views: 13245
- Sat Mar 29, 2003 11:40 am
- Forum: Techniques and Tools
- Topic: sagging element emergency care?
- Replies: 12
- Views: 13245
Sagging elements
You don't need special pins. Just cut and bend some of your own from new element coil...
- Wed Mar 19, 2003 5:38 pm
- Forum: Techniques and Tools
- Topic: Stains from fruit on glass
- Replies: 7
- Views: 10756
Stains from fruit on glass
I've just noticed stains from Bananas on two large fruit bowls. They were made from Spectrum "96" a doule thick clear base with an opal red and opal yellow design on top. The stain is on the opal surface and will not wash off with dish detergent. It is not a coloured stain just slight mark...