Search found 1022 matches

by Tony Smith
Thu Feb 08, 2018 6:57 am
Forum: Techniques and Tools
Topic: Puzzled....
Replies: 2
Views: 5584

Re: Puzzled....

Many people don't realize that the air temperature in the kiln isn't necessarily the same as the glass temperature. The glass temperature is affected by conduction to the mold, convection with the air and radiative coupling to the elements. You're not going to change the air or the mold, so the only...
by Tony Smith
Sun Feb 04, 2018 12:02 pm
Forum: Techniques and Tools
Topic: thicker and thinner together- ok?
Replies: 13
Views: 23116

Re: thicker and thinner together- ok?

The rule of thumb is twice the diameter of the hole from the edge of the hole to the edge of the glass or a minimum of twice the thickness of the glass. I also found a reference to 6 diameters from the corner of the glass. I think your dimensions are very conservative and should work fine. Support y...
by Tony Smith
Thu Nov 30, 2017 6:52 am
Forum: Newcomer Forum
Topic: Sand mold for IN the kiln
Replies: 6
Views: 15689

Re: Sand mold for IN the kiln

Some of the thread talks about hot casting. Then Bert talks about his experience kilncasting: "Many years later, I was taught how to kilncast with sand. That lesson used 20% dry plaster mixed with the sand. I have switched to 25% alumina hydrate, because it lasts longer for me. I reuse my sand ...
by Tony Smith
Tue Nov 28, 2017 6:46 am
Forum: Newcomer Forum
Topic: Sand mold for IN the kiln
Replies: 6
Views: 15689

Re: Sand mold for IN the kiln

This thread from the archives should be helpful.
http://www.warmglass.com/phpBB3/viewtop ... ld#p346214

Tony
by Tony Smith
Sat Aug 19, 2017 9:40 am
Forum: Newcomer Forum
Topic: squares iout of circles
Replies: 6
Views: 11687

Re: squares iout of circles

Jim, Its 0.707 x diameter So if you have a 10" diameter, 10" is the hypotenuse or long side of the square Pythagorean theorem says the square of the hypotenuse of a right triangle equals the sum of the squares of the other sides so, a^2 + b^2 = c^2 c=10, so 10 ^2 = 100 Since a square has e...
by Tony Smith
Wed Aug 16, 2017 8:14 am
Forum: Techniques and Tools
Topic: Firing Top and Sides, etc
Replies: 6
Views: 11111

Re: Firing Top and Sides, etc

The first thing I would do with just a mold or shelf in the kiln, is to measure the max temperature with just the top elements and then just the side elements. Those will be the limiting cases for your testing going forward. I expect you won't get to slumping temperature with just the lid element, s...
by Tony Smith
Fri Aug 04, 2017 6:22 am
Forum: Techniques and Tools
Topic: Adding Switch To RTC-1000
Replies: 10
Views: 14386

Re: Adding Switch To RTC-1000

It's interesting that Olympic is using a single zone of a three-zone controller and wiring all three relays in parallel. I suppose it would allow them to use a single-zone controller without having to change the wiring. To answer your questions, one element has a higher resistance because it is long...
by Tony Smith
Wed Aug 02, 2017 8:39 pm
Forum: Techniques and Tools
Topic: Gasoline-Powereed Sandblasting Compressor Comparisons
Replies: 9
Views: 17317

Re: Gasoline-Powereed Sandblasting Compressor Comparisons

Not exactly... by cycling more frequently, the gas-powered compressor will keep up with the demand, which is your main concern. This doesn't impact compressor life as much as you might think... going from empty to full pressure is way more stressful on a compressor than varying the pressure from 90 ...
by Tony Smith
Wed Aug 02, 2017 5:37 am
Forum: Techniques and Tools
Topic: Gasoline-Powereed Sandblasting Compressor Comparisons
Replies: 9
Views: 17317

Re: Gasoline-Powereed Sandblasting Compressor Comparisons

For their size, gas powered compressors have way more flow than electric, but because they're portable, they have smaller tanks resulting in less reserve capacity. That said, SCFM at pressure is the indicator that you need to evaluate. Depending on your sandblasting setup, you may see some pressure ...
by Tony Smith
Wed Aug 02, 2017 5:28 am
Forum: Techniques and Tools
Topic: Adding Switch To RTC-1000
Replies: 10
Views: 14386

Re: Adding Switch To RTC-1000

It depends if both side relays are wired together as a single zone or if they operate independently. Either way, a DPST toggle switch will do the job. Break one control line on one side of the switch and break the other on the other side of the switch.

Tony
by Tony Smith
Tue Aug 01, 2017 5:52 am
Forum: Techniques and Tools
Topic: Adding Switch To RTC-1000
Replies: 10
Views: 14386

Re: Adding Switch To RTC-1000

The RTC-1000 technical manual is on the Bartlett website. http://www.bartinst.com/kilns/2 On page 5 of the manual is an illustration showing the outputs from the board to the relays. This controller will run three zones. I expect your kiln only has two zones - top and side. To turn off the side elem...
by Tony Smith
Mon Jul 31, 2017 6:08 am
Forum: Techniques and Tools
Topic: Adding Switch To RTC-1000
Replies: 10
Views: 14386

Re: Adding Switch To RTC-1000

It's easy to add two switches, one to control the top (on or off) and another to control side (on or off). It's more of a challenge to combine the two because you need three positions: top; side; and both. You could order a double pole, triple throw switch, they're just not readily available at your...
by Tony Smith
Fri Jun 30, 2017 5:14 am
Forum: Newcomer Forum
Topic: coefficient of expansion
Replies: 2
Views: 6276

Re: coefficient of expansion

It's written in scientific notation. In our world, just read it as 115 +/- 3 or 112 - 118 if you like. It's a much more precise way of writing 115.

Tony
by Tony Smith
Mon May 15, 2017 5:05 am
Forum: Techniques and Tools
Topic: Spectrum System 96
Replies: 6
Views: 10712

Re: Spectrum System 96

jim simmons wrote:Tony.
By "contamination" I assume that you mean the tin left by the float process.
The other Jim
Yup. That's what I meant, and why most people ask which side is up.

Tony
by Tony Smith
Mon May 08, 2017 7:13 am
Forum: Techniques and Tools
Topic: Spectrum System 96
Replies: 6
Views: 10712

Re: Spectrum System 96

Jim is right, but keep in mind that art glass isn't like float glass which has one side "contaminated" by the float process.

Tony
by Tony Smith
Wed Apr 19, 2017 5:32 am
Forum: Techniques and Tools
Topic: Polarizing film
Replies: 11
Views: 15399

Re: Polarizing film

If you bothered to read Jim's reply before being rude to him, you would have understood that he WAS talking about the Rosco product you asked about. Yes, the Rosco film will work. You can use a piece on the light source and another to look through. Jim's suggestion was to use the Rosco film on a lig...
by Tony Smith
Sat Mar 04, 2017 9:26 am
Forum: Techniques and Tools
Topic: metalic stains after blasting
Replies: 6
Views: 10294

Re: metalic stains after blasting

Peter,

Check out Sculpt Nouveau. http://www.sculptnouveau.com

They have a YouTube page as well.

They have patinas and base finishes for all materials that replicate many different oxides.

Tony
by Tony Smith
Thu Feb 16, 2017 6:42 am
Forum: Techniques and Tools
Topic: stencils for sanblasting - photoresist or vinyl cutter
Replies: 27
Views: 60907

Re: stencils for sanblasting - photoresist or vinyl cutter

Seachange, You are correct. The entire sheet would be taped and transferred prior to weeding. The second question gets back to the tack discussion. Larger pieces are much easier to weed off the backing sheet than off glass since the adhesive does stick quite well to glass. Paint mask is a great way ...
by Tony Smith
Tue Feb 14, 2017 7:00 am
Forum: Techniques and Tools
Topic: stencils for sanblasting - photoresist or vinyl cutter
Replies: 27
Views: 60907

Re: stencils for sanblasting - photoresist or vinyl cutter

Seachange, I agree that photoresist is child's play. But it has some detractors that you're already aware of. I haven't found any benefit to using clear transfer tape. I have 6", 12" and 24" rolls of plain old transfer tape (picture light weight masking tape) on the racks and use whic...