Re: Ever seen THIS before?

I sprayed borax on the glass but not while it was in the kiln.
by smallbitz
Sat Jun 16, 2012 1:06 pm
Forum: Techniques and Tools
Topic: Ever seen THIS before?
Replies: 30
Views: 15969

Re: Ever seen THIS before?

No I didn't. Never had to do that before. What temp. Etc. do I prefire at?
by smallbitz
Sat Jun 16, 2012 10:45 am
Forum: Techniques and Tools
Topic: Ever seen THIS before?
Replies: 30
Views: 15969

Re: Ever seen THIS before?

Not sure if this will show very well, but the stuff is even crystalized onto the thermocoupler. It will come off, but strange...
by smallbitz
Sat Jun 16, 2012 10:29 am
Forum: Techniques and Tools
Topic: Ever seen THIS before?
Replies: 30
Views: 15969

Re: Ever seen THIS before?

Yes, it seems to wash off fine. There is devit on the areas where the 'mold/snow' was heavier. I've used the same batch of fiber paper and thinfire as this before. Only new element is the stainless strips. So odd. If I put some of the stainless in my kiln alone to test, how high do I need fire it to...
by smallbitz
Sat Jun 16, 2012 9:24 am
Forum: Techniques and Tools
Topic: Ever seen THIS before?
Replies: 30
Views: 15969

Ever seen THIS before?

This is what I found when I opened my kiln this morning. Looks like it snowed in there! A friend, who was a machinist, gave me a coil of some thin stainless steel (yes, I'm sure it's stainless). I used it to form into a circle (didn't have a mold that size) lined it with thinfire covered 1/8' fiber ...
by smallbitz
Mon Jun 11, 2012 12:40 pm
Forum: Techniques and Tools
Topic: Shard bowl issue
Replies: 11
Views: 6250

Re: Shard bowl issue

I have no idea where this tempered glass came from. It could be 5 or 20 years old...guess I shouldn't depend on it being compatible.
by smallbitz
Mon Jun 11, 2012 8:02 am
Forum: Techniques and Tools
Topic: Shard bowl issue
Replies: 11
Views: 6250

Re: Shard bowl issue

Success! (After many, many tests :-2q(-_-)p) I had to do it in two firings, but I got the look/thickness/and clarity that I was hoping for! Now for my next question.... :lol: I got a lot of tempered glass from a friend (old shower doors) - do I need to keep each piece separated once shattered and us...
by smallbitz
Wed Jun 06, 2012 11:22 am
Forum: Techniques and Tools
Topic: Shard bowl issue
Replies: 11
Views: 6250

Re: Shard bowl issue

Yep, I'm finding that out - can't have it all. I have another test in now adjusting my top temp. Float/tempered glass is new to me, and I haven't had to do this much experimenting in while. I'm actually having a fun/frustrating time with it. Good thing I got the glass for free!! I will not let this ...
by smallbitz
Wed Jun 06, 2012 7:57 am
Forum: Techniques and Tools
Topic: Shard bowl issue
Replies: 11
Views: 6250

Re: Shard bowl issue

Won't I loose the individual 'shards' look (which is what I'm going for) if I fire that high?
by smallbitz
Tue Jun 05, 2012 7:17 pm
Forum: Techniques and Tools
Topic: Shard bowl issue
Replies: 11
Views: 6250

Re: Shard bowl issue

Thanks. That's kind of what I figured...I'll give it a try and see if I get better results. Will the borax spray do any good if I'm not firing above 1400?
by smallbitz
Tue Jun 05, 2012 9:56 am
Forum: Techniques and Tools
Topic: Shard bowl issue
Replies: 11
Views: 6250

Shard bowl issue

In making my shard bowls/plates with tempered glass, I can't seem to get the edges thick enough. I pile the shards up just as thick on the edges (on plate/shallow bowl mold), but for some reason the edges come out like one layer thick and VERY fragile - hardly fused. The middle is perfect. The only ...
by smallbitz
Thu May 31, 2012 5:09 pm
Forum: Techniques and Tools
Topic: Rough Edges...
Replies: 5
Views: 3882

Re: Rough Edges...

I don't have a sandblaster, so I've been trying to do this in one firing (tack/slump). I have carefully sprayed a little borax with a fine mister on the last one I did, but really don't think I used enough. Do I risk much more devit if I fire it twice by tacking and then fusing, or am I better off t...
by smallbitz
Thu May 31, 2012 4:37 pm
Forum: Techniques and Tools
Topic: Rough Edges...
Replies: 5
Views: 3882

Re: Rough Edges...

Thanks, I'll give that a try. Do you think it will make a difference if I overspray it, or am I firing it at too low a temp to matter? I use the borax spray Brad has on the warm tips site.
by smallbitz
Thu May 31, 2012 11:07 am
Forum: Techniques and Tools
Topic: Rough Edges...
Replies: 5
Views: 3882

Rough Edges...

I was given a bunch of tempered glass from a friend who was remodeling her bathroom. Yeah! Never really worked with it before, so it's kind of trial and error (more error #-o ). I seem to have the firing schedule figured out, but can't for the life of me get smooth edges. I pile it up about 1/4"...