Search found 28 matches

by Georgia Novak
Fri Oct 12, 2012 4:30 pm
Forum: Techniques and Tools
Topic: ISO Metal Spinner
Replies: 14
Views: 11219

Re: ISO Metal Spinner

I used a small ss cup, ground off the rolled edge and made the edge as thin as possible then put it over a small clay pot. Pressed down hard to make sure it did not come off, kw it all and presto had a set to fill the kiln and make draped vases. You could do the same with a tall ss cocktail shaker a...
by Georgia Novak
Wed Sep 19, 2012 2:46 pm
Forum: Techniques and Tools
Topic: LIQUID GLASS................CMC.............Alternatives
Replies: 31
Views: 35444

Re: LIQUID GLASS................CMC.............Alternatives

Cynthia: Your stories sound interesting. Are they on your blog? Would love to read them. Georgia
by Georgia Novak
Wed Sep 19, 2012 2:40 pm
Forum: Techniques and Tools
Topic: MESH MELT DISASTER
Replies: 21
Views: 20896

Re: MESH MELT DISASTER

Jim: I see the re-bar but do not know what the mesh is. Is it SS? If so where do you purchase it? Thanks, Georgia
by Georgia Novak
Sun Sep 02, 2012 6:25 pm
Forum: Techniques and Tools
Topic: Wearing gloves when cutting glass
Replies: 17
Views: 27363

Re: Wearing gloves when cutting glass

It sounds like you are cutting at an angle or cutting a lot of textured glass. There is a stick...it is about 8" long x3/4x1", I cann't remember the name of it I've had it for so long. After cutting you run it along the edges and it knocks off all the razor bevels and point spurs. I use it...
by Georgia Novak
Mon Aug 27, 2012 5:01 pm
Forum: Newcomer Forum
Topic: MESH MELT
Replies: 23
Views: 31525

Re: MESH MELT

Immerman of Clear Water Glass Studio uses hardware cloth (Rabbit cage wire) for his wire melts. Isn't that galvanized? Georgia
by Georgia Novak
Thu Aug 02, 2012 4:07 pm
Forum: Techniques and Tools
Topic: how to remove silicone glue?
Replies: 9
Views: 10593

Re: how to remove silicone glue?

Many years ago when I first started stained glass, I glued a panel into the grooved out area of a wooden door, per instructions of teacher. Well, or course a piece broke and the panel had to be removed. I wrote to e-6000 and asked how. They sent me a list in order from weak to strong. I think I fina...
by Georgia Novak
Fri Aug 29, 2003 1:48 am
Forum: Photos and Stuff
Topic: magnet exchange pictures
Replies: 12
Views: 13935

http://www.warmglass.org/participants.html Click on the numbers before each line to see a photo of the magnets. I'll also be putting the "how they were made" info online in the next few da ys. I feel like a real nag, but have not found the "how they were made" info. Maybe I'm lo...
by Georgia Novak
Fri Aug 15, 2003 5:58 pm
Forum: Photos and Stuff
Topic: magnet exchange pictures
Replies: 12
Views: 13935

magnet exchange pictures

I am looking for pictures of the last magnet exchange. Can not find it please help.
Georgia