Search found 114 matches

by Sharol
Fri Oct 04, 2013 11:54 pm
Forum: Newcomer Forum
Topic: haze left after stuck kiln wash is removed
Replies: 8
Views: 10428

Re: haze left after stuck kiln wash is removed

Please post your firing schedule. We need that to best help you understand and troubleshoot what's causing the hazing.
Sharol
by Sharol
Wed Aug 14, 2013 9:47 am
Forum: Photos and Stuff
Topic: Latest Project Completed
Replies: 20
Views: 25756

Re: Latest Project Completed

I just love the edge on this piece. A very interesting composition and very well executed. Bravo, Al!

Sharol
by Sharol
Sat Aug 10, 2013 1:23 pm
Forum: Photos and Stuff
Topic: New Powder Paintings - Landscapes
Replies: 14
Views: 18645

Re: New Powder Paintings - Landscapes

Lovely work! The stand for the mountain landscape is also very, very nice. Did you make it?

Sharol
by Sharol
Sat Jun 01, 2013 7:13 pm
Forum: Photos and Stuff
Topic: Chili hot pepper
Replies: 11
Views: 12314

Re: Chili hot pepper

Those are great! Amazingly realistic. They look exactly like the Fresno Peppers I'm growing in my garden right now! Wonderful color and detail!

Sharol
by Sharol
Wed Apr 17, 2013 9:30 am
Forum: Techniques and Tools
Topic: MELT FUSED INTO CRACKLED PIECE
Replies: 10
Views: 10782

Re: MELT FUSED INTO CRACKLED PIECE

Hi Havi. How thick was the powder in the triangular crackle section? If I am understanding the description of your layup, and depending upon your initial firing speed, the uneven thickness of the glass could have contributed to the break. My approach would be to apply powder to the entire rectangle ...
by Sharol
Sat Feb 09, 2013 9:24 am
Forum: Photos and Stuff
Topic: Navajo
Replies: 25
Views: 27409

Re: Navajo

An absolutely gorgeous piece! Very impressive craftsmanship! Congratulations!
by Sharol
Fri Feb 01, 2013 12:21 pm
Forum: Newcomer Forum
Topic: More about melts
Replies: 9
Views: 9951

Re: More about melts

Hi Havi. I always use a mixture of opaque and transparent glass in my melts. The opaques, especially light colors, seem to help in controlling flow and provides better color separation/distinction. The opaques also help eliminate some of the color shifts that happens with certain warm transparents a...
by Sharol
Wed Jan 30, 2013 11:59 am
Forum: Photos and Stuff
Topic: Colors and Abstraction for Leslie
Replies: 6
Views: 8322

Re: Colors and Abstraction for Leslie

Havi,

That's a beautiful melt. Wonderful colors and clarity.

Sharol
by Sharol
Thu Jan 24, 2013 12:31 pm
Forum: Photos and Stuff
Topic: newest work
Replies: 5
Views: 7542

Re: newest work

Very nice! I love the warm colors and flow of the piece!

Sharol
by Sharol
Thu Jan 24, 2013 12:23 pm
Forum: Art, philosophy, and content
Topic: Chihuly App
Replies: 17
Views: 52753

Chihuly App

It certainly is amazing what those clever application designers are coming up with these days.

Sharol

http://gizmodo.com/5978341/blow-this-ch ... lowing-app
by Sharol
Mon Jan 07, 2013 2:07 am
Forum: Techniques and Tools
Topic: Quick technical question
Replies: 12
Views: 10172

Re: Quick technical question

Les,

I am so sorry this piece is giving you fits. Your "magic" number is almost the same as mine when it comes to reheating difficult pieces. 50 degree ramp is maddening slow, but it works! Best of luck with this.

Sharol
by Sharol
Sat Dec 29, 2012 12:53 pm
Forum: Photos and Stuff
Topic: New work for 2013 shows
Replies: 6
Views: 8332

Re: New work for 2013 shows

I really like the first piece a lot. The way light plays through the center section is very cool and the contrasting wisps are reminiscent of winter clouds. Nicely done!
by Sharol
Thu Dec 06, 2012 2:21 pm
Forum: Photos and Stuff
Topic: Glilt Trip
Replies: 18
Views: 22637

Re: Glilt Trip

Bob,

This is truly lovely. What a great project for you both! Very beautiful.

Congratulations!
by Sharol
Mon Oct 22, 2012 12:45 am
Forum: Photos and Stuff
Topic: Upon the Mere - A New Bowl
Replies: 20
Views: 23190

Re: Upon the Mere - A New Bowl

Thank you...and thanks again Cynthia for your help trouble shooting the slumping issues. Actually, the color composition and design were true collaborations for Vonon and me. It was fun, and a great adventure to share :)

Sharol
by Sharol
Sun Oct 21, 2012 2:08 pm
Forum: Photos and Stuff
Topic: Upon the Mere - A New Bowl
Replies: 20
Views: 23190

Re: Upon the Mere - A New Bowl

Thank you, Janet. It has been so interesting finding ways to incorporate into my pieces the techniques we learned at ob's workshop last fall. It's hard to believe that a year has already passed!

Sharol
by Sharol
Fri Oct 19, 2012 11:10 am
Forum: Techniques and Tools
Topic: Super Spray to fill holes
Replies: 9
Views: 9531

Re: Super Spray to fill holes

Hi Shereen,

I bought the stainless bar through OnLineMetals.com. I bought them in 3 ft and 4 ft lengths (for shipping) and then cut them down to the sizes I wanted. In addition to damming, they come in real handy for aperture and wire melt supports.

Sharol
by Sharol
Fri Oct 19, 2012 1:34 am
Forum: Techniques and Tools
Topic: Super Spray to fill holes
Replies: 9
Views: 9531

Re: Super Spray to fill holes

Hi Vonon, I agree that Super Spray will not give you the fill you need to heal these pits. I suggest filling them with frit/powder and firing to at least a contour fusing temp. I sympathize with the limitation your kiln shelf size imposes (I have this kiln too). It may not be relevant to this discus...
by Sharol
Wed Oct 17, 2012 11:36 am
Forum: Newcomer Forum
Topic: Skutt Hotstart Pro versus Paragon Fusion 6
Replies: 1
Views: 4520

Re: Skutt Hotstart Pro versus Paragon Fusion 6

My 1st kiln was the Skutt HotStart Pro. It has been a workhorse for me and I've had no problems. I've used it regularly for about 8 years. Skutt gives great customer service, including technical assistance. I would suggest though that you seriously consider moving up to the Skutt Firebox 14 or the l...
by Sharol
Wed Oct 03, 2012 1:11 am
Forum: Photos and Stuff
Topic: New colour for bubble.
Replies: 10
Views: 10886

Re: New colour for bubble.

Hi Haydo,

I like this a lot. Can you enlighten me on your title "Truth"? I'd love to hear about your inspiration for this piece.

Sharol
by Sharol
Wed Sep 19, 2012 7:39 pm
Forum: Photos and Stuff
Topic: Upon the Mere - A New Bowl
Replies: 20
Views: 23190

Re: Upon the Mere - A New Bowl

Thank you all for your input! and kind comments! Vonon - It was so interesting to see how the edge turned out on this piece. Without my usual contrasting rim, you can look well into the layers. I very much like the effect and also that the the wire melt sections of the edge retain the textures of th...