by Barry Kaiser
Fri Dec 07, 2012 9:10 pm
Forum: Techniques and Tools
Topic: Screen printing TPI Question
Replies: 25
Views: 25291

Re: Screen printing TPI Question

I do a ton of screen printing. CMC based mediums for screen printing, while they work, are not optimum for screening. These mediums do not hold nearly as much enamel in suspension as pine oil or A-14. Pine oil is a mess to deal with so I only use A-14 (a Thompson product). The results are far superi...
by Barry Kaiser
Thu Dec 06, 2012 9:52 pm
Forum: Techniques and Tools
Topic: hmmmm.....cookie press?
Replies: 3
Views: 4668

Re: hmmmm.....cookie press?

Have tried similar things. The problem is the liquid squeezes out in the first one or two and then you are left with what approaches cement in the gun.

Barry
by Barry Kaiser
Sun Dec 02, 2012 9:04 pm
Forum: Board Help
Topic: Adding photo to private message
Replies: 1
Views: 10332

Adding photo to private message

Brad,
Tried to add a photo attachment to a personal message and got the error massage that the extension jpg was not acceptable.
Any way to add a photo to a personal?

Barry
by Barry Kaiser
Sun Dec 02, 2012 4:12 pm
Forum: Photos and Stuff
Topic: Cave Art
Replies: 17
Views: 16593

Re: Cave Art

Hope the small cracks don't cause a problem. Could be that they actually enhance the texture of the artwork. The piece is too beautiful to lose.
Great use of color!
by Barry Kaiser
Sun Dec 02, 2012 4:08 pm
Forum: Techniques and Tools
Topic: Vitrification on Opal?
Replies: 3
Views: 5139

Re: Vitrification on Opal?

I thought I would put this in this thread. In your case, it sounds like you are just cutting and it really doesn't apply in that case, but here it is anyway. There is a huge difference between "devit" on the top (flat) surface, and the "devit" on the sides of the piece occurring ...
by Barry Kaiser
Fri Nov 30, 2012 1:44 pm
Forum: Photos and Stuff
Topic: New Bowl
Replies: 9
Views: 10101

Re: New Bowl

I like the design and colors,
Don't be shy about posting. Your work is excellent.

Barry
by Barry Kaiser
Thu Nov 29, 2012 11:51 am
Forum: Techniques and Tools
Topic: lettering fused into or onto glass
Replies: 47
Views: 51098

Re: lettering fused into or onto glass

We do lots of screen printing, which would work for this project. But, it is time consuming to make a screen for each name. A far simpler and effective method of doing this is to go to Office Depot or similar store and buy the sets of vinyl letters. Lots of sizes and fonts. If your budget allows, yo...
by Barry Kaiser
Wed Nov 28, 2012 1:04 pm
Forum: Photos and Stuff
Topic: Quiet Sunset
Replies: 14
Views: 14638

Re: Quiet Sunset

Glad you shared it!!


Awesome


Barry
by Barry Kaiser
Fri Nov 02, 2012 7:47 pm
Forum: Techniques and Tools
Topic: Expandable drums
Replies: 17
Views: 22437

Re: Expandable drums

HI Bob,
Just got back into town, so late to this party

I made mine with an arbor from Lortone (about $400) and a local motor from a motor shop($85).
very easy to do.
Drums and wheels added about 250.

Barry
by Barry Kaiser
Tue Oct 09, 2012 2:08 pm
Forum: Techniques and Tools
Topic: LIQUID GLASS................CMC.............Alternatives
Replies: 31
Views: 35445

Re: LIQUID GLASS................CMC.............Alternatives

Jerry,
As a sub for the Flexiglass, try any polyvinyl acetate or Poly-ox based glue such as Elmers, Alenes or Bordens. Mix with a little water to thin some. Use good quality wax paper or treated (for release) aluminum foil. Works quite well.

Barry
by Barry Kaiser
Thu Oct 04, 2012 4:47 pm
Forum: Business Topics
Topic: First Gallery Opening
Replies: 8
Views: 11037

Re: First Gallery Opening

yes Risa,
Relax and enjoy it.
Also go to bbakerinc.com and buy his booth design and Sales CDs. You don't need the jury CD for your situation.

Bruce Baker is the king of common sense when it comes to selling arts and crafts.

Barry
by Barry Kaiser
Sun Sep 23, 2012 7:56 pm
Forum: Photos and Stuff
Topic: Fused glass and 3D printing
Replies: 8
Views: 9955

Re: Fused glass and 3D printing

Very Very cool,

Barry
by Barry Kaiser
Sun Sep 23, 2012 7:53 pm
Forum: Techniques and Tools
Topic: Schedule needed for glass nuggets
Replies: 7
Views: 9270

Re: Schedule needed for glass nuggets

Vicki,
You may need to hold some at 1450.
Check to see if they are done, then turn off the kiln.

Barry
by Barry Kaiser
Thu Sep 20, 2012 8:09 pm
Forum: Photos and Stuff
Topic: Koi
Replies: 4
Views: 5801

Re: Koi

Darn it Valerie,
You keep changing on me. The piece is beautiful, and far different from much of your other work. You keep evolving and consistently for the better

Barry
by Barry Kaiser
Sun Sep 16, 2012 12:41 pm
Forum: Techniques and Tools
Topic: Has anyone used fusion pens from Fusion headquarters?
Replies: 2
Views: 4245

Re: Has anyone used fusion pens from Fusion headquarters?

Try the pilot silver markers...available at Staples (for some reason not available at Office Depot).

Inexpensive and they do withstand firing.

Barry
by Barry Kaiser
Fri Sep 14, 2012 11:54 am
Forum: Jewelry Making
Topic: making consistant small oval cabs
Replies: 7
Views: 12646

Re: making consistant small oval cabs

Another method is to fuse to approximate size and then grind to size and shape. We have a 6 wheel rotary grinder which makes short work of this process.

Barry
by Barry Kaiser
Sat Sep 08, 2012 10:11 am
Forum: Photos and Stuff
Topic: All "eyes" on my website
Replies: 3
Views: 5173

Re: All "eyes" on my website

I have watched your are evolve ever since I found your web site(long ago).
It continues to change with the times. I can't say that it has gotten better, because it has been perfect ever since the beginning. In my opinion, no one can match your personal adornment pieces.

Barry
by Barry Kaiser
Fri Sep 07, 2012 5:09 pm
Forum: Photos and Stuff
Topic: Almost There
Replies: 6
Views: 8078

Re: Almost There

Beautiful and very well done.

Barry
by Barry Kaiser
Fri Aug 31, 2012 10:05 am
Forum: Photos and Stuff
Topic: Sea Urchin
Replies: 19
Views: 21365

Re: Sea Urchin

So Cool!!
by Barry Kaiser
Tue Aug 21, 2012 11:39 pm
Forum: Photos and Stuff
Topic: Cellular
Replies: 20
Views: 22998

Re: Cellular

I guess I could ditto everything posted.
Piece is great