Search found 62 matches
- Sun Jan 11, 2004 1:29 pm
- Forum: Techniques and Tools
- Topic: recycled/float/window glass class recommendation?
- Replies: 7
- Views: 7774
Make a shrine to Bert and worship daily. I have learned so much from Bert on this site that the shrine gets larger all the time. However, I started by assuming float glass does most things at 100 degrees hotter. It is a start, then get a bunch of free windows (I put an ad in the local paper), then g...
- Fri Jan 09, 2004 8:23 pm
- Forum: Techniques and Tools
- Topic: My Glass Got Scum, How Come ?
- Replies: 10
- Views: 10688
borax scum
I also used to get scum occasionally but never do now. In my case, I had used too much borax and it did not all go into solution. So if I would shake the spay bottle before I sprayed, some of the undissolved borax would land on the glass (float) and give me scum. Now I let the borax dissolve and the...