okay so I got the shape I want with the grinder but now..
Moderators: Brad Walker, Tony Smith
okay so I got the shape I want with the grinder but now..
I used a glass grinder to shape the pieces because they looked like blobs (after using a microwave kiln) but now the edges are ugly mat black. now what?
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: okay so I got the shape I want with the grinder but now.
Grind with successively fine sandpaper or diamond pads and water until a luster, then fire polish
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
Re: okay so I got the shape I want with the grinder but now.
Thank you.
What is firepolish? and how do I do it?
What is firepolish? and how do I do it?
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: okay so I got the shape I want with the grinder but now.
Look at the tutorial on the main site www.warmglass.com
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/