Lamp worked rondels and other 2D forms

Post here with questions and topics relating to making glass jewelry.

Moderators: Brad Walker, Tony Smith

Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Lamp worked rondels and other 2D forms

Post by Don Burt »

I do stained glass. I wonder whether shapes like stained glass rondels be made by the lampworking process? I remember from magnet exchanges that I occasionally saw cool lampworked forms that were mostly flat and could be easily encorporated into stained glass window matrices. I think it would be cool to make small (<2") rondels. or little transparent slabs with globby color on them. I know nothing of the process, but I visualize the craft utilizing mostly those colored soda straw rods that I see in people's studios...they don't make sheets of that type of glass for noodling the colored rods onto do they? Do people do this?
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Morganica »

You mean like this?
canepanel.jpg
That's done by snipping a whole bunch of fusing rod and pulled cane "vitrigraph stringer," piling it into a dam and flat-fusing it. I typically compress it instead of dam it, so that I get a thinner-than-6mm piece that's perfectly flat and easily cut.

Not really a rondel, but I like the dimensional qualities. They'd make a cool addition to stained glass.
Attachments
canerollup-8x10.jpg
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Don Burt »

I don't get the vitrigraph thing. I've only seen still photos of people looking up at a drippping kiln with a tongs and shears. I should look up a video of it. People do it with regular BE glass right? Lampworking looks more controllable. But know squat about both processes.
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Morganica »

You stick a bunch of scrap glass, any type as long as it's all compatible, in a flowerpot, drill a hole in the bottom of a little kiln, and put it on stilts. Then you put the flowerpot in the kiln, turn it on and nuke it.

After awhile the glass melts and starts flowing in a stream out the bottom of the pot. You grab it with tongs and manipulate the flow, twisting it or doing whatever. When it cools, you cut the resulting cane into bits.

The stuff in the pic is all Bullseye--the bits that look like bulls eyes literally are the vitrigraph cane. The rest are chopped up rod.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
glasstech
Posts: 6
Joined: Mon Jul 25, 2005 8:26 pm
Location: Delta, BC, Canada

Re: Lamp worked rondels and other 2D forms

Post by glasstech »

That's an interesting technique, Cynthia. Are the bits of rod and cane set on a thin piece of clear sheet before firing to create the clear spaces around the colors?
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Morganica »

You can (and I've done it that way), but typically not--the pieces you chop are generally longer than 6mm, so they're going to spread and fill in the gaps anyway. If you do make them shorter than 6mm, then yep, you'd want to have a base or something to fill in the holes.

This piece was used to make a roll-up--where you give the panel to a glassblower to turn into a vessel--so the pieces were about 10-11mm long. You need the thicker panel to give the gaffer room to expand it. So the base glass wasn't needed at all.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Risa
Posts: 34
Joined: Tue Jul 05, 2011 12:41 pm

Re: Lamp worked rondels and other 2D forms

Post by Risa »

I live in Cincinnati and sometime in the next month or so plan to rent the vitrigraph kiln at our local Bullseye teaching studio. Don, you are welcome to come watch.
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Lamp worked rondels and other 2D forms

Post by rosanna gusler »

Don, just buy the torch. You know you want it. R.
artist, owner of wanchese art studio, marine finisher
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Don Burt »

rosanna gusler wrote:Don, just buy the torch. You know you want it. R.
Yes. I need a kiln with a hole in the bottom too.

Risa, yes. I'd like to watch if by some chance you pick a day that I can get down there. Thank you.
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Lamp worked rondels and other 2D forms

Post by JestersBaubles »

I have a drop bottom kiln that is also used for vitrigraph. So far, I've only used it for raking and making a couple of bracelets. The "users manual" (term used loosely) from the manufacturer mentions nothing about how to set it for vitrigraph, though they included a stainless steel support for the pot. And you really can't find anything on-line. I emailed the rep who sold it to me asking if there was additional information, but that request fell flat :mrgreen: .

I've taken a couple of classes where we watched the instructor pull stringers, but no experience on my own. One of these days I'll get brave enough to say WTF and just do it ;)

Dana
Kate Saunders
Posts: 53
Joined: Thu Mar 18, 2004 10:53 pm

Re: Lamp worked rondels and other 2D forms

Post by Kate Saunders »

Cynthia, to go back a few posts--how do you press the snipped bits of stringer, instead of putting it into a mold? I'd like to work with some of this technique, but I'd like it as thin and as easy to cut as possible. Thanks! Kate
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Morganica »

Kate Saunders wrote:Cynthia, to go back a few posts--how do you press the snipped bits of stringer, instead of putting it into a mold? I'd like to work with some of this technique, but I'd like it as thin and as easy to cut as possible. Thanks! Kate
You lost me there...press the snipped bits of stringer? You mean, do this same thing but with stringer?

Actually, the cane isn't that difficult to cut up to about 3/8 inch in diameter. Much bigger than that, and I get an old mosaic nipper and a hammer. But if you've got a lot of uniformly sized stringer or noodles, you can tape them together like a mini-blind, then hold the sheet down and score across it a few times. Once you've done that you can usually break them apart pretty uniformly. I've got some photos of it in a murrini blogpost:
http://www.morganica.com/glass/fusing/m ... ellyrolls/

I haven't tried that with more than one or two rod at a time; be interesting to see if that works.

It's a pain in the neck to arrange a bunch of (probably jagged-bottomed) stringer or rod or cane--they want to fall over. I typically cut some strips of scrap about a half-inch wide, interleave them to make a frame that's slightly thinner than the length of the pieces. Then I stand the kilnshelf I'm firing on at about a 45-degree angle, rest the glass frame on that, and start filling it up with cut pieces.

Doing it that way lets gravity do most of the work. I can just stick the shelf, frame and all, in the kiln without jostling things around. I usually lay another kilnshelf on top and weight it down so I get a perfectly flat blank.

Is that what you meant?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Valerie Adams »

I pull cane in my studio. I have a Paragon Caldera kiln that I have sitting on a shelf mounted above one of my studio doors (and yes, I lock the door when pulling cane!).
905720_10151343931585683_1286211343_o.jpg
Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Terry Ow-Wing »

Morganica wrote:...
It's a pain in the neck to arrange a bunch of (probably jagged-bottomed) stringer or rod or cane--they want to fall over. I typically cut some strips of scrap about a half-inch wide, interleave them to make a frame that's slightly thinner than the length of the pieces. Then I stand the kilnshelf I'm firing on at about a 45-degree angle, rest the glass frame on that, and start filling it up with cut pieces.

Doing it that way lets gravity do most of the work. I can just stick the shelf, frame and all, in the kiln without jostling things around. I usually lay another kilnshelf on top and weight it down so I get a perfectly flat blank.

Is that what you meant?
Do you have a picture of that? :-k what schedule do you use when you have the murine sandwiched between the two shelves? TIA :) :)
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image
Kate Saunders
Posts: 53
Joined: Thu Mar 18, 2004 10:53 pm

Re: Lamp worked rondels and other 2D forms

Post by Kate Saunders »

Cynthia, Yes! Answers quite a few questions! Thanks, Kate
tob
Posts: 35
Joined: Mon Aug 18, 2003 12:55 pm
Location: Atlanta, GA

Re: Lamp worked rondels and other 2D forms

Post by tob »

Don Burt wrote:I do stained glass. I wonder whether shapes like stained glass rondels be made by the lampworking process? I remember from magnet exchanges that I occasionally saw cool lampworked forms that were mostly flat and could be easily encorporated into stained glass window matrices. I think it would be cool to make small (<2") rondels. or little transparent slabs with globby color on them. I know nothing of the process, but I visualize the craft utilizing mostly those colored soda straw rods that I see in people's studios...they don't make sheets of that type of glass for noodling the colored rods onto do they? Do people do this?
2" rondels would be pretty easy for anyone with decent lampworking skills. Less so for a beginner. It would normally be done with tubing instead of rod, although for that size, one could also use rod and a small blowpipe. If you've ever seen anyone make a lampworked goblet or vase with a foot, a rondel would be made the same way as the foot. Here's a link to a youtube video I found that shows one way to do it using clear boro glass - https://www.youtube.com/watch?v=5LweUhQmvjM

Colored soft glass would be done in a similar way. Extra colors can be added by applying them with frit, powder, or rods. But since many colors soften differently, they can complicate the process of shaping the rondel evenly.

I hope that helps.

The Other Brad
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Lamp worked rondels and other 2D forms

Post by Buttercup »

Don, just thinking out loud here....you have kilns and sandblasting equipment, yes? I've thought about cutting circles of glass, fusing two layers together then sand carving or kiln carving the characteristic swirls into one side....colour to taste. Please try it and tell me if it works! Jen
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Lamp worked rondels and other 2D forms

Post by Don Burt »

I just watched that video that TOB linked. Pretty cool. How much did it cost him to run that torch for seven minutes to make a foot for a goblet I wonder? There's probably more learning curve and infrastructure to managing the flameworking process than I have an appetite for. But Jen, yes, I'm still thinking about kilnforming or potmelting a derivative of spun rondels for use in stained glass panels.
Tod
Posts: 36
Joined: Tue Feb 14, 2006 5:47 pm
Location: Massachusetts

Re: Lamp worked rondels and other 2D forms

Post by Tod »

I guess it's cheating, but I've used feet from thrift store goblets several times. You can fire polish the cut portion in a kiln when needed. Of course, you don't get the dynamic swirls of a hand made rondel but they're mighty cheap!
please visit Beall Glass Studio on Face Book
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Lamp worked rondels and other 2D forms

Post by Buttercup »

Love it, Tod. You could sand carve the swirls before the fire polish. You even have the pontil bump! Thanks, Jen.
Post Reply