okay so I got the shape I want with the grinder but now..

Postby grayeye » Sat Mar 15, 2014 5:33 pm

I used a glass grinder to shape the pieces because they looked like blobs (after using a microwave kiln) but now the edges are ugly mat black. now what?

Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: okay so I got the shape I want with the grinder but now.

Postby Stephen Richard » Sat Mar 15, 2014 6:31 pm

Grind with successively fine sandpaper or diamond pads and water until a luster, then fire polish
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/

grayeye
Posts: 7
Joined: Fri Mar 14, 2014 11:21 pm

Re: okay so I got the shape I want with the grinder but now.

Postby grayeye » Sat Mar 15, 2014 9:23 pm

Thank you.
What is firepolish? and how do I do it?

Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: okay so I got the shape I want with the grinder but now.

Postby Stephen Richard » Sun Mar 16, 2014 8:52 am

Look at the tutorial on the main site www.warmglass.com
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/


Post Reply

Return to “Jewelry Making”

Who is online

Users browsing this forum: No registered users and 1 guest

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com