Hi, we lived abroad for 7 years and I am just now returning to glasswork. My equipment and supplies were in a storage facility without heat or a/c. I fired my first pieces and they all migrated to the middle of the kiln shelf and fused together. I used the Basic 6 schedule from this site BASIC 6-Segment Firing Schedules.
http://system96.com/Resources/FiringGuideFahrenheit.pdf with System 96 glass. I suspect the temp was too high but fear there might be other contributing factors.

I used Thinfire shelf paper that no longer looks white from being in storage so long. It looks beige. Does shelf paper deteriorate?

I used to fire my kilns in my kitchen but have room in the garage in our new house. It was colder (low of 40 F0 and rainy when I fired. Does the garage need to be heated?

Thanks in advance for your kind assistance.

Diane
Attachments
FullSizeRender.jpg
FullSizeRender.jpg (31.33 KiB) Viewed 7087 times

The Hobbyist
Posts: 300
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Help with disaster fire

Postby The Hobbyist » Wed Sep 27, 2017 10:18 am

The old version of thinfire would shrink and curl up. Which may be the cause of your problem since your pieces are small.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg

Vonon
Posts: 191
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Help with disaster fire

Postby Vonon » Wed Sep 27, 2017 12:03 pm

Is there a chance your shelf was stored in such a way that may have allowed it to warp slightly?
Vonon

jim simmons
Posts: 441
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Help with disaster fire

Postby jim simmons » Wed Sep 27, 2017 1:05 pm

Also, you might want to weigh down the edges/corners with some kind of kiln furniture.
This will keep it from curling so much.
The other Jim

dianes
Posts: 5
Joined: Fri Aug 26, 2005 2:53 pm
Location: Fort Collins, CO

Re: Help with disaster fire

Postby dianes » Fri Sep 29, 2017 7:27 pm

Thanks JIM. I will check my self. The kiln furniture is a great idea!

dianes
Posts: 5
Joined: Fri Aug 26, 2005 2:53 pm
Location: Fort Collins, CO

Re: Help with disaster fire

Postby dianes » Fri Sep 29, 2017 7:28 pm

Dang spellcheck. Shelf!

Ed Cantarella
Posts: 153
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Help with disaster fire

Postby Ed Cantarella » Mon Mar 12, 2018 9:51 am

dianes wrote:Dang spellcheck. Shelf!
At least it wasn't elf. :)

BOT - what a drag. :-q(-_-)p All the suggestions above.
Attachments
eecab89039ec15b77cc483c32348d67c.jpg
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.


Post Reply

Return to “Jewelry Making”

Who is online

Users browsing this forum: No registered users and 1 guest

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com