A little warning....
A magless from several years ago - I don't remember which year - just exploded in my kitchen. It didn't fall apart, it detonated sending glass fragments across the room. I heard the 'explosion' 2 floors down. Had I been in the kitchen I would almost certainly have sustained a injury, possibly severe.
The mag was floral - adventurine green and white flower with a blue centre. It was not in direct sunlight, but the room was quite warm.
If you have the same magless you may like to put it somewhere safe!

Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: Danger! Magless! Danger!

Postby Laurie Spray » Sun Aug 18, 2013 10:32 am

Wow.........
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com


Post Reply

Return to “Community Projects”

Who is online

Users browsing this forum: No registered users and 1 guest

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron