Lisa, how easy would it be to cut one of those sheets down? Have you tried it?
Re: Pot Melt Questions ???
It should not be too hard to cut the expanded metal with a small to medium size pair of bolt cutters. Just cut across the sheet one junction at a time on a line at the long end of one of the diamond shaped openings. You may want to file or grind the cut edges to remove any sharp burs to make it easier (safer) to handle.
Best wishes,
Tom in Texas
Best wishes,
Tom in Texas
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
Re: Pot Melt Questions ???
I did try it, but I only have a large pair of tin snips and it was a no go. The stuff I'm getting is pretty heavy and rigid. Bolt cutters might do the trick, as Tom mentioned, but I don't have any.Barbara Muth wrote:Lisa, how easy would it be to cut one of those sheets down? Have you tried it?
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
-
Laurie Saukko
- Posts: 13
- Joined: Tue Mar 13, 2012 12:57 pm
Re: Pot Melt Questions ???
If you know any sheet metal mechanics or heating contractors with their own shop they may be able to help you. 
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Pot Melt Questions ???
If you cant find a shop to help you, you might try to bend the metal and move it back and forth until it breaks..you will need to have a vise or something to hold it rigidly across its length. A hacksaw or Tile saw would work as well.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Re: Pot Melt Questions ???
When you think about it, this is so funny. It's like a think tank full of stoners. No offence, just a warning to other comedians. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!
-
Laurie Saukko
- Posts: 13
- Joined: Tue Mar 13, 2012 12:57 pm
Re: Pot Melt Questions ???
Any large metal fabrication shop will have a shear that can cut it, trust me this is what I do.
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Pot Melt Questions ???
I am missing the beginning of this thread.... 
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie