I found the manufacturers wholesale source for colored micas. It is made by Engelhard. 800-758-9541
The minumum order is $250. Standard packaging is in 25 kilo boxes. I asked the price for gold sparkle mica and was told $14.25 per kilo. They also repackage in 5 kilo and 1 kilo packages with an upcharge. The catalog is on it's way to me with pricing... You can mix and match colors to get the $250. I can see doing a coop order once I understand the selection and pricing.
Lots of companies buy this stuff and mix it in to their products. It looks pretty much identical to Pearlex and the Thompson Lusters. Ferro's Fantasie series seems to be micas like these mixed with a clear flux.
Hidden here on the bottom of this posting LOL is the news that you can fire this stuff on top of enamels and fire the enamel side down and the mica will protect the enamel from sticking to the mold. I did this on prefired fiber paper.
Mica Motherload edit
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Mica Motherload edit
Last edited by Bert Weiss on Fri Feb 13, 2004 11:58 am, edited 1 time in total.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
TonyTony Smith wrote:any idea what the cost of a couple of kilos is? CRLoo is selling a bunch of colored micas for about $45/lb
Tony
I called and discovered that the info I posted wasn't the right place, only a company that sends samples out. I edited the post with better info. I'm waiting for the catalog with pricing.
At $6.48 per lb cost for the raw material repackaging mica looks like a profitable venture at $45 per lb.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Kelly Burke Makuch
- Posts: 37
- Joined: Tue Mar 11, 2003 10:42 pm
- Location: Connecticut
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
-
watercolors4U
- Posts: 3
- Joined: Wed Jan 07, 2004 5:25 pm
Mica Motherload
Hi Ron, It's hard to tell in that photo, but are those mica chips powder or are they about an eight of an inch or smaller in size? I found some by Pearlex I had the other day that were about one eighth of an inch and fused them between two layers of glass. Being new to this I wasn't sure it was OK. I also used some Pearlex powder don't know if that was OK either.
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm