Printing on thin fire
Moderators: Brad Walker, Tony Smith
Printing on thin fire
I am looking for info on printing on thin fire paper and fusing between 96. I have a trophy job and need to include golf club logo? I do not want sepia color....black print would work best,
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Printing on thin fire
Thinfire turns to powder upon firing. You may get the image transferred to the glass, but you will have a pile of powder in between. Transfers can give strong images. You could use vitreous paint or enamels to obtain the image.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
Re: Printing on thin fire
I haven't printed on thinfire but I have drawn an image with a pencil and place it between two pieces of glass and the thinfire stayed white with the image on it.catherine wrote:I am looking for info on printing on thin fire paper and fusing between 96. I have a trophy job and need to include golf club logo? I do not want sepia color....black print would work best,
-
HEIDI in Wa. state
- Posts: 10
- Joined: Tue Jul 26, 2005 12:51 am
- Location: Washington state
Re: Printing on thin fire
I just did a 200 piece trophy order. They also wanted their logo. I screen printed them and they looked great. If you don't have access to that option test the Thinfire method and just make the white a design element.
HEIDI
HEIDI
Re: Printing on thin fire
I have a print gocco silkscreen printer. Which brand of enamel paint would you recommend? is it hard to silkscreen on the glass? The logo would not be more then 2X 2 inches. also does the print need to be capped with clear 96? Thanks for sharing your expert knowledge
-
HEIDI in Wa. state
- Posts: 10
- Joined: Tue Jul 26, 2005 12:51 am
- Location: Washington state
Re: Printing on thin fire
Oh, those print Gocco units are fun! I have used that unit once for printing on glass. I use the Ferro enamels. One word of warning for the print Gocco, wash the screens carefully if you want to reuse them.catherine wrote:I have a print gocco silkscreen printer. Which brand of enamel paint would you recommend? is it hard to silkscreen on the glass? The logo would not be more then 2X 2 inches. also does the print need to be capped with clear 96? Thanks for sharing your expert knowledge
If I can get the picture to load I will post the design I used for the Gocco unit.
Good luck
HEIDI
My Picture is too big-I will try to re-size it...
Last edited by HEIDI in Wa. state on Wed Jun 20, 2012 2:20 pm, edited 1 time in total.
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: Printing on thin fire
Catherine,catherine wrote:I have a print gocco silkscreen printer. Which brand of enamel paint would you recommend? is it hard to silkscreen on the glass? The logo would not be more then 2X 2 inches. also does the print need to be capped with clear 96? Thanks for sharing your expert knowledge
Our Kaiser Glass paints are made to be screen printed. You can adjust the viscosity up with Ferro 3269 or down with A-14. The viscosity is very important to achieve a detailed print.
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com