belts
Moderators: Brad Walker, Tony Smith
-
PDXBarbara
- Posts: 292
- Joined: Sun Mar 09, 2003 4:09 pm
- Location: Portland, OR
belts
Fave cost-effective places to buy silicone carbide belts, 4 x 106?
The Oregon co, Sattex, I used to order from when I shared a belt-sander-equipped studio has dropped its abrasives line. As I recall, their prices were pretty reasonable.
HIS is something like $45 for a box of five 60-grits ($9/each). Grainger has boxes of 25 for like $695 (only looked at 120 grit) which is about $28/belt. Is CRL cheaper? (they won't give me prices without getting at least a DBA.) Yowza. Thanks.
The Oregon co, Sattex, I used to order from when I shared a belt-sander-equipped studio has dropped its abrasives line. As I recall, their prices were pretty reasonable.
HIS is something like $45 for a box of five 60-grits ($9/each). Grainger has boxes of 25 for like $695 (only looked at 120 grit) which is about $28/belt. Is CRL cheaper? (they won't give me prices without getting at least a DBA.) Yowza. Thanks.
Last edited by PDXBarbara on Thu Feb 28, 2013 5:20 pm, edited 1 time in total.
Barbara Bader
Re: belts
HIS requires a dba? you sure?
I found HIS a little more expensive than CRL but much nicer to deal with and worthy of the support.
You could also befriend a local auto/window glass shop and see if they'll "share".
I found HIS a little more expensive than CRL but much nicer to deal with and worthy of the support.
You could also befriend a local auto/window glass shop and see if they'll "share".
-
PDXBarbara
- Posts: 292
- Joined: Sun Mar 09, 2003 4:09 pm
- Location: Portland, OR
Re: belts
noooo. I'd written those sentences out of order. I just edited the damn thing. I'd hoped to catch it before inquiring & famous minds saw it.
Barbara Bader
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: belts
CRL charges me $39.12 for a box of 5 - 120 grit belts (or 220,400). The price drops to $35.85 for 5 boxes. The grits are mixable for the discount.PDXBarbara wrote:Fave cost-effective places to buy silicone carbide belts, 4 x 106?
The Oregon co, Sattex, I used to order from when I shared a belt-sander-equipped studio has dropped its abrasives line. As I recall, their prices were pretty reasonable.
HIS is something like $45 for a box of five 60-grits ($9/each). Grainger has boxes of 25 for like $695 (only looked at 120 grit) which is about $28/belt. Is CRL cheaper? (they won't give me prices without getting at least a DBA.) Yowza. Thanks.
80x costs $41.41, cork belts are $54.72 each, and the rest are $39.12
You must have some bud in the G guild who has an account at CRL.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: belts
Just go in and tell the salesman that you're a glass artist, that you have a CRLaurence wet belt sander and you want an account so you can buy belts. That's how I got my CRL account.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
S.TImmerman
- Posts: 235
- Joined: Wed Nov 25, 2009 9:23 am
- Location: San Diego ,Ca
Re: belts
I check eBay periodically and just bought cl belts (3 boxes of 5) 120 grit for 60.00. I should mention these are NOT from cl account on eBay. But rather an individual who is getting out of glass work. Last week I bought two boxes of 5 (80 grit) from another seller for 34.00. eBay as well as PayPal have excellent buyer protection help if needed. I have had to use it in the past once was paid back in 3 days.
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: belts
Check this one out but you'd have to enquire to get wholesale pricing
http://www.hitechglazing.com/product/43202/40382
http://www.hitechglazing.com/product/43202/40382
-
PDXBarbara
- Posts: 292
- Joined: Sun Mar 09, 2003 4:09 pm
- Location: Portland, OR
Re: belts
I bought mixed-grit assortment of belts from Covingtonhttp://www.covington-engineering.com/index.html recently; great experience and the prices seemed reasonable.
Jerry
-
Doug Randall
- Posts: 102
- Joined: Sun Aug 17, 2003 10:11 pm
- Location: Portland, OR
- Contact:
Re: belts
Barbara. Call me, I've got belts you might be interested in.
Last edited by Doug Randall on Mon Mar 11, 2013 8:28 pm, edited 1 time in total.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: belts
The CRL price of $41.41 is for a box of 5 - 4x106 - 80 grit A discount down to $37.93 is for 5 boxes, mix and match.Doug Randall wrote:Try here: http://www.abrasivesales.com/prodmenu.asp
Good prices and service. (80 grit) 4x106 SiCa belts run about $12.30 each when you buy a dozen.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: belts
Me 2
Jim
Jim
Tony Smith wrote:Just go in and tell the salesman that you're a glass artist, that you have a CRLaurence wet belt sander and you want an account so you can buy belts. That's how I got my CRL account.
Tony