I have a 11" square pattern melt that I had sandblasted with aluminum oxide and refired to eliminate some devit. Well the devit remained on the BE Teal opal sections. If I sift 08 clear powder frit over the entire surface and refire, will it mask the devit?
-
Brad Walker
- Site Admin
- Posts: 1536
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Powder frit to hide devit?
Yes. Just sift it in a very THIN layer, over all of the piece. Fire to full fuse.