I am making some pieces where the base glass is opaque bullseye color, red, blue etc. and it is fired directly onto the fiber paper On the shelf. The opaque glass where it is fired onto the paper is losing its sheen and is Matt and almost has a dusty appearance. Does anyone know why.
Any thoughts on what is causing this and how to prevent it.
Helen
Bullseye fiber paper causing opaque glass to be Matt
Moderators: Brad Walker, Tony Smith
Re: Bullseye fiber paper causing opaque glass to be Matt
Prevent it by using kiln wash. Cheaper and effective.
Re: Bullseye fiber paper causing opaque glass to be Matt
I have been lazy with the paper. I hate it when the opaque glass sometimes stick to shelf and leaves a dent.
Helen Rudy
www.helenrudyglass.com
www.helenrudyglass.com
Re: Bullseye fiber paper causing opaque glass to be Matt
Are you venting the kiln to 1000 degrees?
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Bullseye fiber paper causing opaque glass to be Matt
How hot are you firing?
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Bullseye fiber paper causing opaque glass to be Matt
Are you expecting your base sheet of opal glass to remain glossy on the bottom? That's not going to happen whether you use shelf paper or shelf wash. The bottom of your piece, during a full-fuse process, will pick up the texture of whatever you're firing it on.