Need to know ASAP:
Will BE 1332-50 strike if capped with tekta 3.0- rainbow irid?? or do I need to have the clear on the bottom? I'll full fire to 1480, per your suggested program, with 45 min. hold at 1225.
Capping a fuchsia striker 1332-50
Moderators: Brad Walker, Tony Smith
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Capping a fuchsia striker 1332-50
Yes, it'll strike but the rainbow irid with obscure the color a bit. Although Tekta isn't available with an irid coating as far as I know, so you must be using 1101-0031.
Re: Capping a fuchsia striker 1332-50
Correct..1101-31. Prefer to use clear on top to make tight lines in pieces below. So, fuchsia will fully strike if capped. Thanks!