This glass is supposed to react with silver foil and result in a gold finished look.
Has anyone tried this yet? I bought a piece and don't know what to do with it, so I'd love to see other projects.
Bullseye 1015 - reacts with silver
Moderators: Brad Walker, Tony Smith
-
Kim Manley
- Posts: 17
- Joined: Thu Feb 09, 2012 10:00 am
Re: Bullseye 1015 - reacts with silver
I've seen a box by Nathan Sandberg made with this glass. He brought it to Aus. In October. I don't have a photo but there is clearly a reaction. Bullseye won't ship any to Australia yet so haven't tried it.
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Bullseye 1015 - reacts with silver
There was an artist showing photos of her testing that glass on the FB group called Fused Glass Fanatics.
You can join the group and search for 1015; it'll bring up her photos.
You can join the group and search for 1015; it'll bring up her photos.
-
Brad Walker
- Site Admin
- Posts: 1536
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Bullseye 1015 - reacts with silver
1015 is Reactive Silver Clear. Special production at the present time, but may be in their line down the road.Andrea R wrote:Is 1015 new?
Re: Bullseye 1015 - reacts with silver
Thanks Brad think I will need to get some of that!!!Brad Walker wrote:1015 is Reactive Silver Clear. Special production at the present time, but may be in their line down the road.Andrea R wrote:Is 1015 new?