Hi Everyone!
I have an idea for a mixed-media piece in which I'd like to affix some very thin pate de verre to wood. Is there an adhesive that is best for something like this? I may also consider cold-connections with rivets if it fits in the overall design.
Thanks!
Affixing thin pieces of glass to wood
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Affixing thin pieces of glass to wood
GE Silicon II