Borax or boric acid?
Which is a stronger flux, borax or boric acid?  Are there any other notable differences in the way they work between the two?
			
			
									
						
										
						- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: Borax or boric acid?
All I know is that 20 mule team borax works.  I never tried anything else.  Some will crystalize at the bottom of the bottle, just pour the liquid off and it works.  This stuff is cheap.
			
			
									
						
							Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Borax or boric acid?
borax: Na2B4O7
boric acid: H3BO3
they are not interchangeable and not the same.
			
			
									
						
										
						boric acid: H3BO3
they are not interchangeable and not the same.