Post by Georgia Novak »

A friend gave me many sheets of tempered glass. I know if you hit it hard or brake off a corner it will explode and I have used the crumbles from this.
Now, I am wondering if this great board can give me some ideas of another way to use the glass. She had a store and there are lots of shelves.\
Thanks in advance. Georgia
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Tempered glass

Post by Kevin Midgley »

remove the tempering with a kiln firing and then you can do what you want with it?
Buttercup
Posts: 637
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Tempered glass

Post by Buttercup »

I think Morganica may have shown some gorgeous pieces, bowls etc, made from shattered tempered glass, either here or on her blog. (How's that for being non-commital, sorry but it's a distant memory, or a vivid imagination). Jen
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Tempered glass

Post by Barry Kaiser »

Check with Barbara Cashman.
She teaches several classes using tempered glass. She has been doing so for many many years.