fill weight and firing schedule?
Moderators: Brad Walker, Tony Smith
fill weight and firing schedule?
Does anyone have a fill weight for each cast heart and a firing schedule for this casting mold?
- Attachments
-
- 47140.jpg (38.4 KiB) Viewed 6933 times
Re: fill weight and firing schedule?
Are you wanting them all to be uniform? If not, I just fill until the glass is heaping over.
-
- Posts: 19
- Joined: Wed Feb 22, 2006 10:48 am
- Location: Cambridge, MA
Re: fill weight and firing schedule?
Glass weighs 2.5 times as much as water. Weigh the amount of water that fills a heart and multiply by 2.5 for the amount of glass needed.
-
- Site Admin
- Posts: 1489
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: fill weight and firing schedule?
Alternatively, just fill the mold and fire. Weigh the finished piece. If it's too big, subtract some frit next time. If it's too small, add some frit.Peter McCarthy wrote:Glass weighs 2.5 times as much as water. Weigh the amount of water that fills a heart and multiply by 2.5 for the amount of glass needed.
The firing schedule is more or less a normal full fuse with a slightly longer hold at the top and a longer anneal time.