Post by Judd »

Those of you in the know, does this System 96 glass color strike? If this is the orange I think it is, it color shifts to orange/ brown at fusing temps.

#96-675.5G Godiva
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Does this Color Strike?

Post by Judd »

The pic didn't attach. Sorry.

Nor did it again. Well, the color is easily Google-able. So sorry.
Brad Walker
Site Admin
Posts: 1539
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Does this Color Strike?

Post by Brad Walker »

Probably strikes, most oranges/reds do.