I wanted to add this thin copper 2mm thick twisted copper. into a 5inch diameter glass orb. would the metal cause breakage because too thick. leaf or foil wouldn't give the effect I was looking for.
is there a formula for dimension of metal inclusion vs thickness of glass object?
copper inclusion
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: copper inclusion
2mm is too thick. It will almost certainly crack.
No formula that I'm aware of. It would depend on the particular metal, of course.
No formula that I'm aware of. It would depend on the particular metal, of course.
-
Michael Stevens
- Posts: 83
- Joined: Thu Dec 26, 2019 2:52 pm
Re: copper inclusion
I'm. sorry I meant .2mm
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: copper inclusion
.2mm should be thin enough. Try a small piece as a test.Michael Stevens wrote:I'm. sorry I meant .2mm