Soft fuse with flow?

Postby Mark Wright » Sat Jun 20, 2020 4:29 pm

Looking for help on how to achieve the texture in this picture from Pinterest. So far, I have not been able to reproduce it.
Textured fuse.jpg

Michael Stevens
Posts: 51
Joined: Thu Dec 26, 2019 2:52 pm

Re: Soft fuse with flow?

Postby Michael Stevens » Sat Jun 20, 2020 7:53 pm

Contour fuse should do it. maybe. somewhere between tack fuse and contour fuse temps. the trick is to layer the glass long to short. I use a SS cake pan to. hold the shape while I'm forming.

Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Re: Soft fuse with flow?

Postby Mark Wright » Mon Jun 22, 2020 9:38 am

Thanks for the hints. Based on your comment of using a cake pan it appears it also needs to be dammed. I'll give it a try.

Michael Stevens
Posts: 51
Joined: Thu Dec 26, 2019 2:52 pm

Re: Soft fuse with flow?

Postby Michael Stevens » Mon Jun 22, 2020 10:06 am

I use the cake pan to create the shape, don't need to cook it in that pan if you want organic and varied length. but I prefer even edge, I line the pan with kiln paper

Don Burt
Posts: 536
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: Soft fuse with flow?

Postby Don Burt » Mon Jun 29, 2020 2:44 pm

are those edges of strips or stringers?

Marty
Posts: 851
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Soft fuse with flow?

Postby Marty » Mon Jun 29, 2020 7:08 pm

Don- it's strips on edge, cut in different widths so some will flop and flow. Watching the kiln is crucial until you know what happens when- you want the stuff stuck firmly to itself and the edges rounded nicely.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 12 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com