sgraffito again
Moderators: Brad Walker, Tony Smith
sgraffito again
P.S sorry, but I dont want to use just powdered frit on its own, I'll make too much of a mess doing it for the first time.!
-
Brad Walker
- Site Admin
- Posts: 1540
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: sgraffito
You can use either powdered frit or enamel/paint. Generally, we use powder dry and paint with a binder. I guess you could use wet powder, but not sure that's any easier or less of a mess than dry powder.raphy wrote:For any of you who do sgraffito, do you use powdered frit or paint. If you use frit do you mix it with aloe to paint it on. I was taught years and years ago but have completely forgotten. Thank you for any help.
Re: sgraffito again
Thank you, if you use the powder binded or not how many layers?
-
Brad Walker
- Site Admin
- Posts: 1540
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: sgraffito again
The number of layers depends on the darkness of the powder, but in general we use about 4 grains thick.raphy wrote:Thank you, if you use the powder binded or not how many layers?