Here's another stupid Question...
Moderators: Brad Walker, Tony Smith
-
skin_mechanic
- Posts: 35
- Joined: Fri Mar 26, 2004 10:42 pm
- Location: Birmingham, AL
Here's another stupid Question...
...Here it goes: What is the process for tempering glass? I tried a google search on it, but found next to nada 
Re: Here's another stupid Question...
Briefly, you heat up glass in a chamber, then rapidly cool it by blasting it with air.Skin_Mechanic wrote:...Here it goes: What is the process for tempering glass? I tried a google search on it, but found next to nada
This makes a type of "skin" on the glass.
The outside is in compression, and the interior is in tension.
( I just changed the above, I had it reversed)
If you break the skin, by impact, or sandblasting too deeply, bang!
Last edited by Brock on Sat Apr 03, 2004 9:40 pm, edited 1 time in total.
My memory is so good, I can't remember the last time I forgot something . . .
-
skin_mechanic
- Posts: 35
- Joined: Fri Mar 26, 2004 10:42 pm
- Location: Birmingham, AL
-
Susan Moore
- Posts: 96
- Joined: Mon Oct 06, 2003 10:07 pm
- Location: Austin, TX
- Contact:
[quote="Skin_Mechanic"]Ok, now your bein' a (information)tease
I need the specifics: How high do I need to fire the piece? How much does it need to be cooled? Is it cooled down to room temp, or only to below the strain point? And what's the difference between heat strengthening and fully tempered?[/quote
Nah, I wasn't teasing, you can't temper in your kiln. You can't even heat treat, (think coke bottles, or marbles). All we can do is anneal, take all the stress out. Leaving controlled stress in glass requires expensive industrial equipment. Brock
Nah, I wasn't teasing, you can't temper in your kiln. You can't even heat treat, (think coke bottles, or marbles). All we can do is anneal, take all the stress out. Leaving controlled stress in glass requires expensive industrial equipment. Brock
My memory is so good, I can't remember the last time I forgot something . . .
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
You can't do it without a major investment in equipment. The trick is to heat the glass up above anneal and cool it back to room temperature in less than 30 minutes without shattering the glass. Done correctly ( I think Bert mentioned 600 horsepower blowers), the glass heats up uniformly from all sides and cools quickly but uniformly leaving a skin that has very high stresses on the surface from shrinking faster than the core.Skin_Mechanic wrote:Ok, now your bein' a (information)teaseI need the specifics: How high do I need to fire the piece? How much does it need to be cooled? Is it cooled down to room temp, or only to below the strain point? And what's the difference between heat strengthening and fully tempered?
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
skin_mechanic
- Posts: 35
- Joined: Fri Mar 26, 2004 10:42 pm
- Location: Birmingham, AL
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
A tempering furnace costs a zillion dollars. The heating chamber has expensive alumina rollers that move the glass back and forth while it is being heated from both sides. 3/8" glass takes 5 minutes to heat up from room temp to 1100ºF. Then it is rolled in to the quench part of the furnace which is powered by a 750 HP blower. The blower directs cold air through nozzles placed every few inches on top and bottom. If the glass is going to break it does so about 2 minutes in to the quench. There is a sizeable pile beneath the quench in a removable bin. The cooling part of the process takes 7 minutes, so 12 minutes to go from room temp to 1100 and back down to room temp. Of course there are no guarantees that your kiln fired glass will survive the process.
Once I learned what not to do, I have not lost any pieces. I believe that my glass is likely much better annealed than sheet glass from the factory, so my percentages should be better.
An interesting factor is that the thicker the glass, the easier a challenge it is to temper it. The big HP is necessary for thinner glasses. I still never heard of anybody who managed to do it on the cheap.
Brock explained the stress thing. Glass is very strong in a state of compression, stronger than steel. We know all too well how weak it is in tension, though
Once I learned what not to do, I have not lost any pieces. I believe that my glass is likely much better annealed than sheet glass from the factory, so my percentages should be better.
An interesting factor is that the thicker the glass, the easier a challenge it is to temper it. The big HP is necessary for thinner glasses. I still never heard of anybody who managed to do it on the cheap.
Brock explained the stress thing. Glass is very strong in a state of compression, stronger than steel. We know all too well how weak it is in tension, though
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions