Peg
Posts: 74
Joined: Tue Apr 08, 2003 7:50 am
Location: Bristol, UK

Silver leaf effect

Postby Peg » Fri May 23, 2003 8:49 am

I have fused gold leaf in a 'Bullseye sandwich' with good results - now I want a silver equivalent. Of course silver leaf itself will merely stain the glass yellow - any ideas as to what I can use to get a metallic silver leaf effect? Is there such a thing as platinum leaf?

Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Postby Barbara Muth » Fri May 23, 2003 9:56 am

yes, and palladium as well, although neither will give you the same effect that silver can. If you use silver leaf under irridized glass or unde Bullseye's "crystal clear" (I forget the stock number) you should get the silver without any staining.

Barbara
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS

Brad Walker
Site Admin
Posts: 1346
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Postby Brad Walker » Fri May 23, 2003 9:57 am

A good quality silver foil will stay silver. Bullseye sells a foil that will work.

Paul Bush
Posts: 52
Joined: Sun Mar 09, 2003 3:59 pm
Location: Portland, Oregon

Postby Paul Bush » Fri May 23, 2003 11:21 am

I use Bullseye's silver foil under their regular clear all the time, and have had no yellowing.

Paul
Paul Bush
Flying Fish Studio
Portland, Oregon

Strega

Postby Strega » Fri May 23, 2003 3:35 pm

I think the only problem you MIGHT have is if you are not sandwitching it or take the temp too high. I include old broken jewelry in my fuses sometimes, and it generally doesn't change if it is "captured".


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Eric Bloom, Google [Bot] and 44 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com