Kiln Repair Cement Help

Postby Randy W » Tue May 27, 2003 12:49 pm

The front edge of my kiln is a bit torn up from me jammin stuff in there to prop the lid open when I'm drying my kiln shelves. I'm pretty sure that's where the white crumbs are coming from that end up on my pieces. I bought a 1 pound jar of kiln repair cement to smooth over the rough spots. It mentions in the directions that you can dilute the cement with water and apply to the lid to keep dust from falling. It doesn't mention how much to thin it or how to go about applying it and drying it. Just let it air dry? For how long? Or close the lid and turn on the kiln to dry it? Does anyone have any experience with this stuff thry're willing to share?

Thanks, Randy

Cynthia

Postby Cynthia » Tue May 27, 2003 1:13 pm

I diluted mine to be thin enough to apply with a brush....so it was pretty darn watery. It is cement, so the gook will separate out and you need to keep stirring while applying. Keep it off of your elements. I've heard some say they put newspaper over the elements to protect them, then just fired the paper off. I simply avoided getting it on the elements.

I let mine dry for a day, then fired up to 500 with a hold just like for primer to drive out what water remained, then fired as usual. I did this well over two maybe three years ago and haven't had any more problems with brick bits falling into my work.

Darrin Strosnider
Posts: 16
Joined: Tue Mar 11, 2003 10:33 am
Location: Desert Southwest

Postby Darrin Strosnider » Tue May 27, 2003 1:26 pm

Interesting. I wonder if this would work for the element grooves in the lid too... I'm tempted to pull my elements out of my lid and apply it to the grooves- this is where my "crumbs" come from.

Kitty
Posts: 437
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Postby Kitty » Tue May 27, 2003 1:39 pm

i've got a front-loading cress, and have repaired the front edge of the bricks with kiln cement a few times. the cement works, but eventually it breaks down and crumbles off. for that reason i wouldn't want to put it on the lid. impending doom. there was a post in the last month or two about other materials to encase elements and correct the problem of particles falling. maybe someone else remembers that thread more precisely. it might have been about a foam spray that hardened up ... sorry i can't recall the details. kitty.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 35 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com