haze as well slumping large shallow pieces

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Jeri D
Posts: 65
Joined: Fri Mar 28, 2003 8:43 pm
Location: Martha's Vineyard.MA

haze as well slumping large shallow pieces

Post by Jeri D »

After my beginner early bubbles, i have returned to bigger and bolder. Now something new. On slumping both a 14" round(clear with confetti and stringers, also red w/ pattern bar) ) they both hazed on the underside in the slump except for the middle, where there is slight bubbling too.
I can't find where I mislaid my schedule, so help me there too.
Does a slow slide on a shallow mold cause this? Is it picking up kiln wash. Inquiring fuser wants to know :?
Jeri from MV
Post Reply