Graham Stone's Firing Recipes

Postby Terrie Corbett » Wed Jun 04, 2003 12:27 am

:?: I haven't seen anything about Graham Stone in a while. On the old website (in December '02) I checked the appropriate box indicating that I would like to buy his firing recipe book when it became available to website users again. (there was the option to buy from the website or directly from him). I have never heard anything else about it. Are they no longer available through the website? If not, does someone have information where it can be purchased? Any help would be appreciated.

Thank you.

Terrie

Brad Walker
Site Admin
Posts: 1346
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Postby Brad Walker » Wed Jun 04, 2003 12:57 am

Graham's book is very hard to find. From time to time he sends me a few (I have a standing order for as many as he will send), but he hasn't sent any copies in months. I don't know any place to get the book (Whitehouse doesn't even have it), but you MAY be able to track down a very expensive copy through Artisan Books in Australia. The book is still listed in their catalog at $126 Australian (about $85, plus shipping from down under) http://www.artisan.com.au/

I keep hoping Graham will give me permission to print a US edition, but no luck yet.

Brian and Jenny Blanthorn
Posts: 353
Joined: Mon Mar 10, 2003 5:25 pm
Location: UK
Contact:

Postby Brian and Jenny Blanthorn » Wed Jun 04, 2003 4:11 am

Brad Walker wrote:Graham's book is very hard to find. From time to time he sends me a few (I have a standing order for as many as he will send), but he hasn't sent any copies in months. I don't know any place to get the book (Whitehouse doesn't even have it), but you MAY be able to track down a very expensive copy through Artisan Books in Australia. The book is still listed in their catalog at $126 Australian (about $85, plus shipping from down under) http://www.artisan.com.au/

I keep hoping Graham will give me permission to print a US edition, but no luck yet.


Anything on what Graham is up 2 now ??
Image


Post Reply

Return to “Techniques and Tools”