schedule for "fire polish"
Posted: Thu Jun 05, 2003 1:57 pm
I need to "fire polish" some 2x2 single layer squares for a mosaic wall project.
We have all the 2x2 multi layer tiles done. this is the program I used for the multi layer tiles. Someone from this site gave it to me and I worked great.
600 1480 20
9999 970 20
120 850 0
200 700 0
off
the kids at school have loved working with the glass. I will post pictures as soon and I have the wall done.
We have a large skutt, programable kiln at school (work) and I have small manual kiln at home.
Thanks, KRIS
We have all the 2x2 multi layer tiles done. this is the program I used for the multi layer tiles. Someone from this site gave it to me and I worked great.
600 1480 20
9999 970 20
120 850 0
200 700 0
off
the kids at school have loved working with the glass. I will post pictures as soon and I have the wall done.
We have a large skutt, programable kiln at school (work) and I have small manual kiln at home.
Thanks, KRIS