Borax Spray

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
tom suter
Posts: 55
Joined: Sun Mar 09, 2003 8:12 pm
Location: springfield il
Contact:

Borax Spray

Postby tom suter » Fri Mar 14, 2003 10:55 am

I am getting ready to fire a 1/4" float and a post warn me to be sure I use borax. I have never use this. I am going to be putting frit on top of this should I spray the borax over the project after I get the frit in place or just on the the float. :?: Thnaks for the help

Glenda Kronke
Posts: 64
Joined: Tue Mar 11, 2003 11:44 am
Location: Austin, TX
Contact:

Postby Glenda Kronke » Fri Mar 14, 2003 11:03 am

Is the frit 'float compatable'? I use float glass all the time and spray with Fusemaster clearcoat overspray with no devit problems. I always put tin side down for double safety.
glenda

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Postby Bert Weiss » Fri Mar 14, 2003 1:33 pm

Tom

The recipe for borax spray is in the old archoives many times. I think it may have been put in FAQ or tutorial. Making your own is cheap and easy.

You can get away with spraying before or after doing your frit work. It depends on what you are doing with the frit. If you were covering the entire surface with frit, you probably don't need it, but if the frit is in patches you probably will.

Bert


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 28 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron