Need basic help on preparing to slump simple project....

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
candala
Posts: 28
Joined: Tue Mar 25, 2003 7:44 am

Need basic help on preparing to slump simple project....

Post by candala »

I've never slumped before. I want to slump a small vase with some dichroic. Do you FIRST have to fire the glass (fuse) before slumping? Also, how do you determine the exact size and shape to place over the mold? Is there a slumping for idiots tutorial or video I can get my hands on? Thanks.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Need basic help on preparing to slump simple project....

Post by jim simmons »

candala wrote:I've never slumped before. I want to slump a small vase with some dichroic. Do you FIRST have to fire the glass (fuse) before slumping? Also, how do you determine the exact size and shape to place over the mold? Is there a slumping for idiots tutorial or video I can get my hands on? Thanks.
You might check out the tutorial at this site. 8)