Postby cheryl kumiski » Thu Aug 14, 2003 11:16 am

i was using 1/4" grinder bits to make holes in plates so they would accept clock works. the problem being 1 bit equals 3 holes. yikes!!! and i can't figure out how to use a drill press without electrocuting myself. my kingdom for a solution!!

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Postby Brock » Thu Aug 14, 2003 11:18 am

Ask Susan Taylor Glasgow! Brock
My memory is so good, I can't remember the last time I forgot something . . .

Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Postby Barbara Muth » Thu Aug 14, 2003 11:23 am

Cheryl, there is a lot of discuission on drilling holes and drill bits in the old archives. You might find your solution there.

Barbara
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS

starchimes (Andrea)
Posts: 26
Joined: Tue May 20, 2003 11:39 am
Location: Dallas, TX
Contact:

Postby starchimes (Andrea) » Thu Aug 14, 2003 11:52 am

Try getting your bits at http://www.lopacki.com. The prices are good. Bits last a good while. I can usually get about 50 holes per bit.

Regards,
Andrea

paulajane

Postby paulajane » Thu Aug 14, 2003 1:42 pm

I purchased some bits that would not work with my flexible shaft set up. So we bought a cheap $20 drill press stand at Harbor Freight Tools and then adapted it to hold a cordless battery operated a drill. To keep it going steadily we slide a tie wrap over the button because battery operated drills do not have buttons to press to keep them going continuously. It works great.

Paula

cheryl kumiski
Posts: 9
Joined: Fri Jul 18, 2003 1:55 pm
Location: chuluota, florida
Contact:

Postby cheryl kumiski » Thu Aug 14, 2003 2:09 pm

paulajane wrote:I purchased some bits that would not work with my flexible shaft set up. So we bought a cheap $20 drill press stand at Harbor Freight Tools and then adapted it to hold a cordless battery operated a drill. To keep it going steadily we slide a tie wrap over the button because battery operated drills do not have buttons to press to keep them going continuously. It works great.

Paula

thanks paula--this seems the most effective. i did check the archives and most of the info concerns a dremel tool. since i need a 1/4" hole drilled through 6 layers of glass the dremel isn't an option. i'll try a regular drill with diamond bits.
cheryl

cheryl kumiski
Posts: 9
Joined: Fri Jul 18, 2003 1:55 pm
Location: chuluota, florida
Contact:

Postby cheryl kumiski » Thu Aug 14, 2003 2:10 pm

Brock wrote:Ask Susan Taylor Glasgow! Brock

how??

cheryl kumiski
Posts: 9
Joined: Fri Jul 18, 2003 1:55 pm
Location: chuluota, florida
Contact:

Postby cheryl kumiski » Thu Aug 14, 2003 2:11 pm

starchimes wrote:Try getting your bits at http://www.lopacki.com. The prices are good. Bits last a good while. I can usually get about 50 holes per bit.

Regards,
Andrea

thank you!! will do.
cheryl

Dick Ditore
Posts: 58
Joined: Mon Mar 10, 2003 12:56 pm
Location: San Diego, Ca
Contact:

Postby Dick Ditore » Thu Aug 14, 2003 2:59 pm

Harbor freight also sells diamond coring bits in small sizes. I have used the 1/2" and the 1". I use my bench drill press. You have to lubricate. I bought a suction ring at cr laurence, and fill with water. Go easy and no problem. I have cut up to 1 3/8" holes.


Dick

Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Postby Paul Tarlow » Thu Aug 14, 2003 4:15 pm

Brock wrote:Ask Susan Taylor Glasgow! Brock


...saw that one coming

Alecia Helton
Posts: 108
Joined: Mon Aug 25, 2003 12:35 am
Location: outside of Dallas TX

Making holes

Postby Alecia Helton » Mon Aug 25, 2003 1:21 pm

Sorry to be a late reply. I just joined the list.

I bought my drill press at Home Depot, the drill was included with the press. I buy the hollow-core diamond bits from Rio Grande.

To drill with water: I place a large plastic lid on the base plate to protect the metal from from the wet sponge that lays on top of it. I use a squirt bottle to keep the drill and glass wet.

There are times when you really need three hands. And I have used my chin at times, but I've never feared electrocution.

Hope this helps. :)

Alecia
Alecia Helton
Wear Original Wonders!
Carrollton TX


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 19 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com