Looking for a tutorial...

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
daffodildeb
Posts: 125
Joined: Mon Jul 28, 2003 3:48 am
Location: Hot Springs Village, AR

Looking for a tutorial...

Post by daffodildeb »

I'm looking for a tutorial that appeared as a link in this forum (I think) about a week or so ago. It showed how to make a frame that scrap glass could be placed into, brought to a really molten state, and the glass would drip down through some sort of mesh onto a shelf, all nicely swirled as it dripped. :!:

Can anyone help me find that tutorial? I've looked in the search files, but really didn't have a good title to help in the hunt.
Deb
Dick Ditore
Posts: 58
Joined: Mon Mar 10, 2003 12:56 pm
Location: San Diego, Ca
Contact:

Post by Dick Ditore »

try pot melt, or look for posts by rob morey.

Dick
Nelson Tan
Posts: 41
Joined: Sun Mar 09, 2003 9:23 pm
Location: Manila
Contact:

Post by Nelson Tan »

Hi I believe I saw that too in the Photos Board

nelson
Rob Morey
Posts: 76
Joined: Sun Mar 09, 2003 4:33 pm
Location: San Diego
Contact:

Post by Rob Morey »

Is this what you're talking about?

http://www.ramoreydesign.com/shelfmelt.html

Rob
"Come to the edge. We might fall. Come to the edge. It's too high! Come to the edge! And they came, and he pushed...... and they flew."
-- Christopher Logue
daffodildeb
Posts: 125
Joined: Mon Jul 28, 2003 3:48 am
Location: Hot Springs Village, AR

Post by daffodildeb »

Yes, yes, YESSSSS...

Thanks so much--it answers some questions only a photo can do. Excellent tutorial, BTW.

Now to make one for myself! I bought hi-temp wire for it today.
Deb
Post Reply