Hi, I am using spectrum 96, have done 2 firings. The first was the blank, the second to place small geometric tiles in design. I plan to decorate on top of this design using noodles I have cut in half and formed into shapes using a torch. My question is, If I want the noodles to retain their shape and not go to a full fuse (technically tack fuse I guess) can I "fuse" them and slump at the same time?
Shari
PattyJohnson
Posts: 11
Joined: Sat Mar 22, 2003 1:43 am
Location: Wisconsin
Contact:

Post by PattyJohnson »

Hi Shari,
yes you can tack them during a slump...I usually apply a little glue to keep them from moving.

http://plj.alternateversion.com/images/ ... SERIES.JPG[/img]

not sure if the pic worked

Take care...Patty Johnson
http://www.pljglassart.com
Judith Andre
Posts: 28
Joined: Thu Mar 20, 2003 2:38 am
Location: Lincoln, NE

Post by Judith Andre »

Patty...Where do you get your iron plate holders? I like the simplicity of them.
Judith
Judith
Nancy Juhasz
Posts: 113
Joined: Sun Mar 09, 2003 10:10 pm
Location: Ohio

Post by Nancy Juhasz »

Question here. When I slump can I tack fuse 1/8 in glass to the base of what I am slumping or draping? I was under the impression that the tack fuse had to be a separate step. It would be wonderful if I could eliminate one firing.